CGPCO

4 / 5

12Cr1MoVG Boiler Tube Seamless Diameter 219.1x12.7

stars, based on 0reviews
7items available

GB5310 chinese standard 12Cr1MoVG seamless steel tubes and pipes for high pressure boiler.

Equivalent: ASTM A335 P11/ASME A213 T11

 Application

Used in petroleum, chemical, electric power, boiler industry with high temperature resistance, low temperature resistance, corrosion resistance seamless steel pipes


Chemical component:

Grade

Chemical component(mass fraction)/%

C

Si

Mn

Cr

Mo

V

P

S

Max

12Cr1MoVG

0.08-0.15

0.17-0.37

0.40-0.70

0.90-1.20

0.25-0.35

0.15-0.30

0.025

0.010

 

Mechanical property:

Grade

Tensile property

impact absorbed energy

Strength of extension

MPa

REL

Percentage elongation after fracture   A/%

Lengthways

Crosswise

Lengthways

Crosswise

No less than

12Cr1MoVG

470-640

255

21

19

40

27

 

Test:

- Flattening Test (D﹥22mm-400mm and S≤40mm);

- Bending Test (D﹥400mm or S﹥40mm);

- Flaring Test (D≤76mm and S≤8mm);

- Macro test;

- Nonmetallic inclusion;

- Grain size;

- micro structure;

- Decarburized Layer;

- Inter-granular corrosion test;

- Surface quality inspection;

- Nondestructive testing.

Size available

OD*WT: 8~406.4mm*6-100mm


Inaddition, my company have these tube stock about 3000tons, so the delivery is very fast. one or two weeks is enough.


My company hot sale steel pipe:

 ASTM A106 B seamless pipes,(1” to 24” sch40, sch80),

API 5L GR.B steel pipes, (seamless pipe, LSAW pipe, SSAW pipes, 1” to 110” sch 40, sch80),

Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),

ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160)

Recent Reviews
+