CGPCO
API 5CT P110 Casing 13 3/8" 72 PPF BTC R3
API 5CT P110 Casing Tubing is a API 5CT Oil Casing Pipe & mainly used for oil well drilling. We manufacture API 5CT J55 Casing Tubing in accordance with the API 5CT standard, it is available as short thread type and long thread type supplied with their couplings.
According to American Petroleum Institute Standard API SPEC 5CT1988 1st edition, the steel grade of API 5CT oil casing pipe can be divided into ten types, including H-40, J-55, K-55, N-80, C-75, L-80, C-90, C-95, P-110 and Q-125. We supply the casing pipe & API 5CT J55 Casing Tubing accompanied with thread and coupling, or we offer our product in accordance with the following forms for option.
API 5CT Casing Tubing Chemical Composition, Mass Fraction (%)
| Group | Grade | Type | C | Mn | Mo | Cr | Ni max. | Cu max. | P max. | S max. | Si max. | ||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| min. | max. | min. | max. | min. | max. | min. | max. | ||||||||
| 1 | 2 | 3 | 4 | 5 | 6 | 7 | 8 | 9 | 10 | 11 | 12 | 13 | 14 | 15 | 16 |
1 | H40 | - | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - |
- | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - | ||
- | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - | ||
1 | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - | ||
Q | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - | ||
R95 | - | - | 0.45 c | - | 1.9 | - | - | - | - | - | - | 0.03 | 0.03 | 0.45 | |
2 | M65 | - | - | - | - | - | - | - | - | - | - | - | 0.03 | 0.03 | - |
1 | - | 0.43 a | - | 1.9 | - | - | - | - | 0.25 | 0.35 | 0.03 | 0.03 | 0.45 | ||
9Cr | - | 0.15 | 0.3 | 0.6 | 0.9 | 1.1 | 8 | 10 | 0.5 | 0.25 | 0.02 | 0.01 | 1 | ||
13Cr | 0.15 | 0.22 | 0.25 | 1 | - | - | 12 | 14 | 0.5 | 0.25 | 0.02 | 0.01 | 1 | ||
C90 | 1 | - | 0.35 | - | 1.2 | 0.25 b | 0.85 | - | 1.5 | 0.99 | - | 0.02 | 0.01 | - | |
T95 | 1 | - | 0.35 | - | 1.2 | 0.25 d | 0.85 | 0.4 | 1.5 | 0.99 | - | 0.02 | 0.01 | - | |
C110 | - | - | 0.35 | - | 1.2 | 0.25 | 1 | 0.4 | 1.5 | 0.99 | - | 0.02 | 0.005 | - | |
3 | e | - | - | - | - | - | - | - | - | - | - | 0.030 e | 0.030 e | - | |
4 | Q125 | 1 | - | 0.35 | 1.35 | - | 0.85 | - | 1.5 | 0.99 | - | 0.02 | 0.01 | - | |
| a The carbon content for L80 may be increased up to 0.50 % maximum if the product is oil-quenched. b The molybdenum content for Grade C90 Type 1 has no minimum tolerance if the wall thickness is less than 17.78 mm. c The carbon content for R95 may be increased up to 0.55 % maximum if the product is oil-quenched. d The molybdenum content for T95 Type 1 may be decreased to 0.15 % minimum if the wall thickness is less than 17.78 mm. e For EW Grade P110, the phosphorus content shall be 0.020 % maximum and the sulfur content 0.010 % maximum. NL = no limit. Elements shown shall be reported in product analysis. | |||||||||||||||
API 5CT Casing Tubing Tensile And Hardness Requirements
| Group | Grade | Type | Total elongation under load % | Yield strength MPa | Tensile strength min. MPa | Hardness a max. | Specified wall thickness mm | Allowable hardness variation b HRC | ||
|---|---|---|---|---|---|---|---|---|---|---|
| min. | max . | HRC | HBW | |||||||
| 1 | 2 | 3 | 4 | 5 | 6 | 7 | 8 | 9 | 10 | 11 |
| 1 | H40 | - | 0.5 | 276 | 552 | 414 | - | - | - | - |
J55 | - | 0.5 | 379 | 552 | 517 | - | - | - | - | |
K55 | - | 0.5 | 379 | 552 | 655 | - | - | - | - | |
N80 | 1 | 0.5 | 552 | 758 | 689 | - | - | - | - | |
N80 | Q | 0.5 | 552 | 758 | 689 | - | - | - | - | |
R95 | - | 0.5 | 655 | 758 | 724 | - | - | - | - | |
| 2 | M65 | - | 0.5 | 448 | 586 | 586 | 22 | 235 | - | - |
L80 | 1 | 0.5 | 552 | 655 | 655 | 23 | 241 | - | - | |
L80 | 9Cr | 0.5 | 552 | 655 | 655 | 23 | 241 | - | - | |
L80 | 13Cr | 0.5 | 552 | 655 | 655 | 23 | 241 | - | - | |
C90 | 1 | 0.5 | 621 | 724 | 689 | 25.4 | 255 | ≤ 12.70 12.71 to 19.04 19.05 to 25.39 ≥ 25.40 | 3.0 4.0 5.0 6.0 | |
T95 | 1 | 0.5 | 655 | 758 | 724 | 25.4 | 255 | ≤ 12.70 12.71 to 19.04 19.05 to 25.39 ≥ 25.40 | 3.0 4.0 5.0 6.0 | |
C110 | - | 0.7 | 758 | 828 | 793 | 30 | 286 | ≤ 12.70 12.71 to 19.04 19.05 to 25.39. ≥ 25.40 | 3.0 4.0 5.0 6.0 | |
| 3 | P110 | - | 0.6 | 758 | 965 | 862 | - | - | - | - |
| 4 | Q125 | 1 | 0.65 | 862 | 1034 | 931 | b | - | ≤ 12.70 12.71 to 19.04 ≥ 19.05 | 3.0 4.0 5.0 |
| a In case of dispute, laboratory Rockwell C hardness testing shall be used as the referee method. b No hardness limits are specified, but the maximum variation is restricted as a manufacturing control in accordance with 7.8 and 7.9 of API Spec. 5CT. | ||||||||||
API 5CT Casing Tubing Steel Color Code
| Name | J55 | K55 | N80-1 | N80-Q | L80-1 | P110 |
|---|---|---|---|---|---|---|
| Casing | a bright green band | two bright green bands | a bright red band | a bright red band + a green band | a red band + a brown band | a bright white band |
| Coupling | entire green coupling + a white band | entire green coupling | entire red coupling | entire red coupling + a green band | entire red coupling + a brown band | entire white coupling |
Available Sizes: 2 3/8″, 2 7/8″ and 3 ½” Outer Diameter
Macaroni Tubing: 1 1/4 “ – 2 1/16” Nom.
Grades: J55, J55, N80, L80, P110
End Finishing: External Upset Ends (EUE), PH6 (and equivalent connections), Flush Joint, Integral Joint (IJ)
Specialties:
Threading
Heat treating
External upset
Drifting (Full-length, or just ends)
Hydrostatic Testing
Full third-party inspection capabilities (EMI, SEA, and Weld Line)
Couplings – EUE, AB Modified, turned down, special clearance couplings
Coating to customer specifications
Pup Joints
Hot Tags:
Seamless boiler tube EN 10216-2 P265GH size: out diameter 21.3-219.1mm, China, suppliers, factory, cheap price, discount, bulk, customized, seamless pipe 42CrMo, aviation fuel transmission seamless pipe, ssaw welded pipe for oil conveying, ssaw pile pipe astm a252, carbon steel seamless pipe sour service