ASTM A210 A1 Seamless Boiler Tube

stars, based on 0reviews
6items available

SA 210 A1 Ferritic Steel Boiler Tube is Primarily Used For Heat Exchanger Tubes In Critical Thermal Power Plants And Waste Heat Recovery Boilers Operated In The Temperature Range Of 300°C -400 °C. ASTM 210 A1 Ferritic Steel Pipes Are Fitted In Water Walls Operating At Temperatures Around 300-400°C .These Steels Tubes Are Exposed In The Furnace To High Temperature. Both Corrosion And Erosion Attack From The Hot Flue Gas Stream Significantly Enhances The Higher Metal Wastage Rate.


ASTM A210 / A210M Grade A-1 Chemical Compositions

Chemical Components (%)
GradeCSiMnPSMoCrV
A-1≤0.27≥0.10≤0.93≤0.035≤0.035///

ASTM A210 / A210M Mechanical Tests Required

Mechanical Properties
GradeTensile


Strength (Mpa)

Yield


Strength (Mpa)

Elongation


(%)

Hardness

(HRB)

A-1≥415≥255≥30≤79

 

ASTM A210 / A210M Tube Wall Thickness Tolerance

Seamless, Cold-Finished Tubes

Outside Diameter

In. (mm)

Wall thickness Tolerance %
Over (+)Under (-)
1 ½ (38.1) and under200
Over 1½ (38.1)220

ASTM A210 / A210M Tube Outside Diameter Tolerance

Cold-Finished Seamless Tubes

Outside Diameter

In. (mm)

Permissible Variations In. (mm)
Over (+)Under (-)
Under 1 (25.4)0.004 (0.10)0.004 (0.10)
1 to 1 ½ (25.4 to 38.1), Incl0.006 (0.15)0.006 (0.15)
Over 11⁄2 to 2 (38.1 to 50.8), Excl0.008 (0.20)0.008 (0.20)
2 to 21⁄2 (50.8 to 63.5), Excl0.010 (0.25)0.010 (0.25)
21⁄2 to 3 (63.5 to 76.2), Excl0.012 (0.30)0.012 (0.30)


Specification Of ASTM A210 ASME SA210 GRADE A1 Seamless Tubes

Standard: ASTM A210 / ASME SA210

Description Name: ASME SA210 / ASTM A210 boiler pipes, ASTM A210 seamless tubing, ASTM A210 cold drawn seamless steel tubes

Size: 1⁄2 in. to 16 in. 

W.T.: 1.5mm-50mm

Shape: Round

Production Type: Hot finished and cold finished.

Length: Single random length/ Double random length or as customer’s actual request max length is 13 m

Grade: Grade A-1

Heat Treatment: Hot-finished tubes need not be heat treated. Cold- finished tubes shall be given a subcritical anneal, a full anneal, or a normalizing heat treatment after the final cold finishing process.



ASTM A210 A1 Seamless Boiler Tube

ASTM A210 A1 Seamless Boiler Tube

ASTM A210 A1 Seamless Boiler Tube

ASTM A210 A1 Seamless Boiler Tube


Hot Tags: astm a210 a1 seamless boiler tube 3in xs 10-12m length, China, suppliers, factory, cheap, price, discount, bulk, customized, seamless pipe en10305, cold drawn small size seamless tube, ssaw welded pipe for constrcution, stainless steel plate astm a480, ssaw welded pipe, lsaw welded pipe x70