CGPCO
ASTM A519 4140 Cold Drawn Seamless Tube 3" SCH 80, SCH160
ASTM A519 Steel Seamless Tube Materials & Manufacture
Steel used to produce A519 steel tube may be made by any process; if the purchaser requires a specified type of melting, please note this in your RFQ or when ordering. A519 tubes must be made in a seamless process and either hot finished or cold finished, as specified.Chemical Requirements For A519 Seamless Steel Tubing
Steel Grade And Chemical Composition (%) Of ASTM A519:
Grade | C | Mn | P≤ | S≤ | Si | Cr | Mo |
| 1008 | ≤0.10 | 0.30-0.50 | 0.040 | 0.050 | - | - | - |
| 1010 | 0.08-0.13 | 0.30-0.60 | 0.040 | 0.050 | - | - | - |
| 1018 | 0.15-0.20 | 0.60-0.90 | 0.040 | 0.050 | - | - | - |
| 1020 | 0.18-0.23 | 0.30-0.60 | 0.040 | 0.050 | - | - | - |
| 1025 | 0.22-0.28 | 0.30-0.60 | 0.040 | 0.050 | - | - | - |
| 1026 | 0.22-0.28 | 0.60-0.90 | 0.040 | 0.050 | - | - | - |
| 4130 | 0.28-0.33 | 0.40-0.60 | 0.040 | 0.050 | 0.15-0.35 | 0.80-1.10 | 0.15-0.25 |
| 4140 | 0.38-0.43 | 0.75-1.00 | 0.040 | 0.050 | 0.15-0.35 | 0.80-1.10 | 0.15-0.25 |
Mechanical Properties Of ASTM A519:
| Grade | Condition | MPa Tenslle Point | Yield Point | Elongation |
| 1020 | CW | ≥414 | ≥483 | ≥5% |
| SR | ≥345 | ≥448 | ≥10% | |
| A | ≥193 | ≥331 | ≥30% | |
| N | ≥234 | ≥379 | ≥22% | |
| 1025 | CW | ≥448 | ≥517 | ≥5% |
| SR | ≥379 | ≥483 | ≥8% | |
| A | ≥207 | ≥365 | ≥25% | |
| N | ≥248 | ≥379 | ≥22% | |
| 4130 | SR | ≥586 | ≥724 | ≥10% |
| A | ≥379 | ≥517 | ≥30% | |
| N | ≥414 | ≥621 | ≥20% | |
| 4140 | SR | ≥689 | ≥855 | ≥10% |
| A | ≥414 | ≥552 | ≥25% | |
| N | ≥621 | ≥855 | ≥20% |
Please note the meaning of below abbreviation in table 2:
HR----Hot Rolled
CW----Cold Worked
SR----Stress Relieved
A----Annealed
N----Normalized


Hot Tags: cold drawn seamless tube 1045 material, China, suppliers, factory, cheap, price, discount, bulk, customized, seamless pipe for gas transmission, fire sprinkler pipe, pipe stock, aviation fuel transmission seamless pipe, astm a312 tp310s stainless steel tube for heat exchanger, seamless tube for low temperature environment