EN10297-1 34CRMO4 GAS CYLINDER TUBE

34CrMo4 is an alloy structural steel with high endurance and creep strength at high temperatures. It's mainly used for cylinder manufacturing or structural parts working under high loads such as transmission parts of vehicles and engines; turbine-generator rotor, spindle, heavy load drive shaft, large section parts, locomotive traction gear, supercharger transmission gear, rear shaft, connecting rod and spring clamp with great load, can also be used for the oil drilling pipe joints and fishing tools below 2000m. However, its poor weldability requires preheating before welding, heat treatment after welding and stress elimination. It is generally used after quenching and tempering, and used after high and medium frequency surface quenching or quenching and low and medium temperature tempering. 


Outer diameter:89mm-368mm

Wall thickness:4-18 mm

length:5.8-12m

Straightness: Deviation 2 mm/m max.

Delivery allowance: +/- 10%

Size Tolerance:

Length toleranceWT toleranceO.D. tolerance 
0/+100mm for a total length+0,9mm -1 / +1%


Chemical Composition:

C

Si

Mn

P

S

Cr 

Mo 

0.30~0.37

0.10~0.40

0.60~0.90

≤0.035

≤0.035

0.90~1.20

0.15~0.30


Mechanical Values :

Grade

Tensile strength Rm

Yield strength YS

Elongation A(%)

34CrMo4

≥985(100)

≥835(85)

≥12


UT protocol according to ISO 10893-10

Non-destructive control: flux leakage acc. To EN 10246-4

Internal transversal defects- level severity F3

External transversal defects- level severity F2

flux leakage acc. To EN 10246-5

Internal longitudinal defects: level severity F3

External longitudinal defects: level severity F2

Mechanical tests will be done on samples at simulated heat treatment

conditions oil quenching at 880°C /30 minutes and tempering at 650°C /30 minutes.

Mill Test Certificate: EN 10204 3.1

Inspection: Bureau Veritas Acceptable

Packing: In bundles 2.5MT max, pipe ends with protection caps

Protection: No outside/inside coating, protecting material required

34CrMo4 is the alloy material commonly used in EN 10297-1 standard and the heat treatment is mainly normalizing or annealing. My company supply 34CrMo4 seamless steel pipes in various sizes and specifications even the size hard to find. We provide a high-pressure steel pipe for many industries.


Alloy Gas Cylinder Seamless Tube EN10297-1 34CrMo4 Size: OD 356 Mm X9.53 Mm. Length: 11-12m Length.

Alloy Gas Cylinder Seamless Tube EN10297-1 34CrMo4 Size: OD 356 Mm X9.53 Mm. Length: 11-12m Length.

Alloy Gas Cylinder Seamless Tube EN10297-1 34CrMo4 Size: OD 356 Mm X9.53 Mm. Length: 11-12m Length.

Alloy Gas Cylinder Seamless Tube EN10297-1 34CrMo4 Size: OD 356 Mm X9.53 Mm. Length: 11-12m Length.


Hot Tags: alloy gas cylinder seamless tube en10297-1 34crmo4 size: od 356 mm x9.53 mm. length: 11-12m length., China, suppliers, factory, cheap, price, discount, bulk, customized, low temperature seamless pipe, gb/t9711 ssaw pipe, erw line pipe, seamless pipe asme gb5310, gi coil zinc coated, api 5l ssaw spiral pipe

Recent Reviews
+