Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length

stars, based on 0reviews
7items available

API Standard Specification For Seamless Line Pipe

The American Petroleum Institute specification API 5L addresses seamless and welded steel line pipe for pipeline transportation systems in the petroleum and natural gas industries.  API 5L is suitable for conveying gas, water, and oil.  

Specifications for API 5L adhere to the International Organization for Standardization ISO 3183, standardizing pipeline transportation systems within the materials, equipment and offshore structures for natural gas, petroleum, and petrochemical industries.  When authoring the standards, the technical committee recognized that there are two basic Product Specifications Levels (PSL) of technical requirements and therefore developed PSL 1 and PSL 2.  PSL 1 is a standard quality for line pipe where PSL 2 contains additional chemical, mechanical properties, and testing requirements. 

Grades covered by this specification are A25, A, B and "X" Grades X42, X46, X52, X56, X60, X65, X70, and X80.  The two digit number following the "X" indicates the Minimum Yield Strength (in 000's psi) of pipe produced to this grade.


Standard                                            API 5L 

Product Specification Level             PSL-2 

Steel grade                                         X52

Chemical Properties %

PSL

C, a

   Mn a

P

       S

 Si

V

Nb

Ti

Other

CEIIW

CEpcm

1

0.24

1.40

0.025

0.015

0.45

0.10

0.05

0.04

b,c

.043

0.025

2

0.28

1.40

0.03

0.03

-

b

b

b

-

-

-

 Mechanical Properties        

                                                                        API 5L PSL-1 X52                API 5L PSL-2 X52

Tensile strength, min /max, psi (MPa)         66,700(460)/ n/a                      66,700 / 110,200 

Yield strength, min /max, psi (MPa)            52,000 (300)/n/a                      52,000 / 76,900

  1. a.      For each reduction of 0.01% below the specified maximum concentration for carbon, an increase of 0.05% above the specified maximum concentration for manganese is permissible, up to a maximum of 1.65% for > grades B, but < X52; up to a maximum of 1.75% for grades >X52, but <X70; and up to a maximum of 2.00% for grade X70

  2. b.      The sum of the niobium, vanadium, and titanium concentrations shall be < 0.06%.

  3. c.       Unless otherwise agreed, 0.50% maximum for copper, 0.30% maximum for nickel, 0.30% maximum for chromium, and 0.12% maximum for molybdenum.

Select differences between PSL 1 and PSL 2:


PSL1PSL2

CVN impact (Charpy) testingNone requiredRequired for all grades
Nondestructive inspection of seamlessOnly when purchaser specifies   SR4SR4 mandatory
CertificationCertificates when specified per SR15Certificates (SR 15.1) mandatory
TraceabilityTraceable only until all tests are passed, unless SR15 is specifiedTraceable after completion of tests (SR 15.2) mandatory



Hydrostatic TestRequiredRequired

Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length

Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length


Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length

Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length

Carbon Steel Seamless PipeAPI 5L X52 PSL2 16in SCH80 12m Length


Hot Tags: carbon steel seamless pipeapi 5l x52 psl2 16in sch80 12m length, China, suppliers, factory, cheap, price, discount, bulk, customized, seamless tube asme sa213, 457mm diameter seamless line pipe, seamless pipe en 10210, erw welded steel pipes diameter 711mm, astm a335 p5 alloy seamless pipe, alloy steel plate en 10083