CGPCO

4 / 5

DIN 2448 St 44.0 Seamless steel Pipe 12" SCH160 12M

stars, based on 0reviews
7items available


DIN 2448 is a standard which gives specifications for carbon steel pipes and tubes that are seamless in nature. It includes weights, masses per unit length, couplings, and dimensions. The din 2448 pipe cannot be hot formed with or without consequent heat treatment


DIFFERENCES IN CHEMICAL COMPOSITION

Standard

Grade

Chemical Composition %

C

Mn

P

S

Si

Cr

Cu

Ni

Mo

V

ASTM A106

B

≤0.30

0.29-1.06

≤0.035

≤0.035

>0.10

≤0.40

≤0.40

≤0.40

≤0.15

≤0.08

ASTM A53

B

≤0.30

≤1.20

≤0.05

≤0.045

–

≤0.40

≤0.40

≤0.40

≤0.15

≤0.08

API 5L

B(PSL-1)

≤0.28

≤1.20

≤0.030

≤0.030

–

–

–

–

–

–

DIN 1629,
DIN 2448

St 37.0

≤0.17

–

≤0.040

≤0.040

–

–

–

–

–

–

St 44.0

≤0.21

–

≤0.040

≤0.040

–

–

–

–

–

–

EN10210

S235JRH

≤0.17

≤1.40

≤0.040

≤0.040

–

–

–

–

–

–

GB/T8163,
GB/T8162

10#

0.07-0.13

0.35-0.65

≤0.035

≤0.035

0.07-0.37

≤0.15

≤0.25

≤0.30

–

–

20#

0.17-0.23

0.35-0.65

≤0.035

≤0.035

0.17-0.37

≤0.25

≤0.25

≤0.30

–

–

DIFFERENCES IN MECHANICAL PROPERTIES

Standard

Grade

Tensile Strength
 (MPa)

Yield Strength
 (MPa)

Trans.Elongation
     (%)

Impact Test
  (J)

ASTM A106

B

>415

≥240

≥16.5

–

ASTM A53

B

>415

≥240

–

–

API 5L

B(PSL-1)

>414

≥241

As clause a

–

DIN 1629

St 37.0

350-480

≥235

≥23

–

DIN 2448

St 44.0

420-550

≥275

≥19

–

EN10210

S235JRH

360-510

≥235

≥26

27 (+20°C)

GB/T 8163

10#

335-475

≥205

≥24

–

GB/T 8162

20#

410-550

≥245

≥20

–

  We can produce special diameter and wallthickness seamless pipes. Adopted standards: ASTM A106, ASTM A53, API 5L GR.B, GB/T8163,EN10216 etc

  The diameter range from 1000m to 1600m, wallthickness from 20- 400mm. The pipes are extensively applied for nuclear power station and other key project.


My company hot sale stainless steel pipe:

 TP304/304L, TP316/TP316L, stainless steel welded and seamless pipes, (1” to 48” sch10, sch20, sch40, sch80),

TP321, TP347 stainless steel seamless pipes, (1/2”to 24” seamless)

Recent Reviews
+