CGPCO

4 / 5

EN 10297-1 Grade 20MnV6 Carbon Steel Tube 152X25mm 9-12m

stars, based on 0reviews
7items available

EN 10297-1 Grade 20MnV6 Carbon Steel Seamless Tubes are low-cost Low Carbon Steel Tubes with 016-022 % carbon content with combination of 130-170 % manganese easy to form and shape. EN 10297-1 Grade 20MnV6 Tubes are available in sizes, thicknesses, diameters and specifications to suffice the clients’ piping system requirements. Carbon Steel EN 10297-1 20MnV6Tubing thoroughly examined on numerous quality stages before final dispatch.

Carbon Steel EN 10297-1 Grade 20MnV6 Tubes has a number of other excellent features to provide like having reliable, superior finish, affordable and more.EN 10297-1 Grade 20MnV6 Carbon Steel Seamless Tubes, EN 10297-1 Grade 20MnV6+QT Tubes and EN 10297-1 Grade 20MnV6+N Seamless Tubes are manufactured with great precision utilizing premium quality raw material and sophisticated technology.

20MnV6 is a carbon-manganese steel micro alloyed with vanadium, generally supplied in the black hot rolled condition with a typical tensile strength range of 600 - 790 Mpa and a high typical yield strength range of 440 - 570 Mpa.Characterized by excellent machinability due to silicon - calcium treatment and precise control of the sulphur content, excellent weldability with high yield and tensile strengths due to the micro - alloying effect of the vanadium.The low carbon content and the vanadium addition allows surface hardening by carburising, carbonitriding or nitriding. It will also respond to high or medium frequency induction hardening and can be through hardened and tempered producing a moderate improvement in tensile and yield strength, this varying depending upon wall thickness. 20MnV6 seamless tube is used extensively by all industry sectors for a wide range of applications utilizing.


EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m
Chemical Composition of 20MnV6
EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m  EN 10297-1 Grade 20MnV6 Carbon Steel Tube   152X25mm   9-12m

Min. %Max %
Carbon0.160.22
Silicon0.100.35
Manganese1.301.60
Vanadium0.080.15
Phosphorous00.03
Sulphur0.020.04
Mechanical Property Requirements - As Supplied in the Black Hot Rolled Condition of 20MnV6 20MV6
Tensile Strength Mpa Min.
Wall Thickness (mm)
<16620
<25310
>25550
0.2% Yield Strength Mpa Min.
Wall Thickness (mm)
<16470
<25460
<30430
<40420
<50410
<70400
Elongation % Min18
Hardness Brinell Min180
 
Product Name:
20MnV6 alloy seamless tube
Material:
Carbon steel,alloy steel 
Standard&Grade:
EN10297-1, SAE4130
Manufacture Method:
Cold Drawn, Hot rolled
Internal Surface Treatment:
Honing, Skiving&roller burnishing
Size Range:
ID of 168mm max for cold drawing, ID of 500mm for hot rolled.
Delivery Condition:
,Annealed,Normalized,Quenched+Tempered
End finish:
Plain  ends with square cuts,free of burrs

My company hot sale seamless steel line pipes:

 ASTM A106 B seamless pipes, API 5L GR.B seamless steel pipes(1” to 24” sch40, sch80),

API 5L X52, X65, X70 PSL2 seamless line pipe (2” to 24” sch40, sch80, sch160),

Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),

ASTM A333 GR.6 seamless pipes,

Recent Reviews
+