CGPCO

4 / 5

EN10028 P265GH Seamless boiler Pipe 4” SCH160 10-12M

stars, based on 0reviews
7items available

EN10028-2 covers alloy and no-alloy steels for pressure vessels with elevated temperature properties. P265GH is useful at moderate temperatures for pressure purposes. At the standard thickness it has a minimum yield strength of 265 MPa. It is normalised by heating through the thickness of the plate to a temperature between 890 to 950°C without holding.


P265GH is a weldable non-alloy quality pressure vessel steel. P265GH has a wide application in the manufacture of pressure vessels, boilers and heat exchangers in the oil and gas industry.P265GH is also used in chemical and pharmaceutical process plants. 

P265GH seamless steel tube pipe carbon contents is 0.13%. P265GH seamless steel tube pipe used in  gas and oil transportation, mechanical and manufacture, steel structure, boiler, ship building, bridging, automobile chassis.



P265GH Chemical Composition

Grade

C

Si

Mn

Mn(Min)

P

S

Al

N

Cr

Cu

Mo

Nb

Ni

Ti

V

CR+Cu+Mo+Ni

P265 GH

0.2

0.4

1.4

0.8

0.025

0.01

0.02

0.012

0.3

0.3

0.08

0.02

0.3

0.03

0.02

0.7

P265GH Physical Properties

Yield Strength

≤ 16

16 < t ≤ 40

40 < t ≤ 60

60 < t ≤ 100

100 < t ≤ 150

150 < t ≤ 250

265

255

245

215

200

185

Tensile Strength

≤ 100

100 < t ≤ 150

150 < t ≤ 250

410 to 530

400 to 530

390 to 530

Elongation after Fracture % Min

22

Impact Energy

-20

0

+20

27J

34J

40J

It has some heat resistance but for higher temperatures and applications where corrosion is more of a factor then chrome moly steels are recommended. P265GH is specified in EN 10028-2:2009 which replaces the old BS 1501 and DIN17155 standards. It is a steel for use as boiler plate with  a minimum yield strength of 265 MPa. P265 is normally delivered in the normalized condition.


P265GH seamless pipe available:
 Out Diameter:17.2mm~273mm
 Thickness:1.8mm~40mm

Hot Tags: seamless pipe P265GH, China, suppliers, factory, cheap, price, discount, bulk, customized, st37 seamless tube 88.9mm diameter, seamless pipe a106 b normal use, astm a335 p11 alloy seamless pipe, seamless pipe p265gh, 20mnv6 seamless tube diameter 152mm, seamless pipe

Recent Reviews
+