CGPCO

4 / 5

EN10219 S355J0 ERW Welded Pipe 16in Diameter STD 12m

stars, based on 0reviews
7items available

S355J0 Welded Steel Pipes

 

S - stands for structural steel
355 - stands for minimum yield strength (though it will vary based on thickness, refer below section for more details)
Normally S355 will have following variation based on impact strength at different temperatures, as steel become more brittle when temperature drops. If your structure need to withstand -20°C, it's better and safer to choose S355J2. 
 
S355JR - Can withstand an impact energy of 27J at +20°C
S355J0 - Can withstand an impact energy of 27J at 0°C
S355J2 - Can withstand an impact energy of 27J at -20°C
S355K2 - Can withstand an impact energy of 27J at -30°C (40J at -20°C)

 

S355J0 Characteristic

 

S355J0 is a low carbon, high tensile strength structural steel which can be readily welded to other weldable steel. 

With its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in normalized or controlled rolling condition.

 

 S355J0 Application 

 

Structural application in freight cars, transmission towers, dump trucks, cranes, trailers, bull dozers, excavators, forestry machines, railway wagons, dolphins, penstocks, pipes, highway bridges, building structures, oil and gas platforms, offshore structures, shipbuilding, power plant, palm oil equipments and machineries, fans, pumps, lifting equipments and port equipments.

 

 

S355J0 Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, Q+T, N+T, TMCP, Z15, Z25, Z35

 

 

S355J0 Chemical Composition(max %)

 

 

EN

Chemical Composition

C

Si

Mn

Cr

Mo

Ni

V

N

S

P

CU

S355J0

0.24

0.60

 1.70

-

-

-

-

0.014

 0.040

0.040

0.60

 

S355J0 Mechanical Properties:

Thickness (mm)

Yield Strength Reh

min (N / mm²)

Tensile Strength Rm

min (N / mm²)

Elongation A5 min

(%)

Impact Values Charpy-V-Notch Longitudinal

Average from 3 Speimens Thk.

>10<150mm.

3<thk<100

315-335

490-630

max 22

27 Joules at 0 C

 

  • Available sizes: 2 3/8 in. – 30 in. outer diameter (OD)

  • Grades:  S355 serious

  • Specifications:  ASTM  A53-B, EN10219, API-5L

  • Coating/Overlay Options: Fusion Bonded Epoxy, TGF-3, PowerCrete / Abrasion-resistant overlay (ARO), and other customer-specific coatings

  • End Finishing: Plain-end beveled (PEB) for welding; Zap-Lok

  • Wall Thicknesses: Light Wall, Standard Wall, Extra Heavy and other wall thickness available

 

EN10219 S355J0 ERW Welded Pipe 16in Diameter STD 12m

EN10219 S355J0 ERW Welded Pipe 16in Diameter STD 12m

EN10219 S355J0 ERW Welded Pipe 16in Diameter STD 12m

 

 

 

 

Hot Tags: s355 erw welded pipe 16in diameter std 12m length, China, suppliers, factory, cheap, price, discount, bulk, customized, alloy steel plate en 10083, erw welded precision pipe, ssaw welded pipes l415m, erw pipe gb/t3091, aisi 4130 seamless mechanical tube, seamless pipe astm a 179

Recent Reviews
+