CGPCO

4 / 5

LSAW Weld Pipe ASTM A691 1 1/4 Cr 22" SCH80 12M Length

stars, based on 0reviews
7items available
ASTM A691 / A691M - 09 Standard Specification For Carbon And Alloy Steel Pipe, Electric-Fusion-Welded For High-Pressure Service At High Temperatures

This specification2 covers carbon and alloy steel pipe, electric-fusion-welded with filler metal added, fabricated from pressure-vessel-quality plate of several analyses and strength levels and suitable for high-pressure service at high temperatures. Heat treatment may or may not be required to attain the desired mechanical properties or to comply with applicable code requirements. Supplementary requirements are provided for use when additional testing or examination is desired.


Pipe steel Grade

Pipe GradeType of SteelASTM SpecificationHB, max
NumberGrade
CM-65carbon-molybdenum steelA204/A204MA201
CM-70carbon-molybdenum steelA204/A204MB201
CM-75carbon-molybdenum steelA204/A204MC201
CMSH-70carbon-manganese-silicon steel, normalizedA537/A537M1
CMS-75carbon-manganese-silicon steelA299/A299M——
CMSH-80carbon-manganese-silicon steel, quenched and temperedA537/A537M2
1/2 CR1/2 % chromium, 1/2 % molybdenum steelA387/A387M2201
1 CR1 % chromium, 1/2 % molybdenum steelA387/A387M12201
1 1/4 CR1 1/4 % chromium, 1/2 % molybdenum steelA387/A387M11201
2 1/4 CR2 1/4 % chromium, 1 % molybdenum steelA387/A387M22201
3 CR3 % chromium, 1 % molybdenum steelA387/A387M21201
5 CR5 % chromium, 1/2 % molybdenum steelA387/A387M5225
9 CR9 % chromium, 1 % molybdenum steelA387/A387M9241
919 % chromium, 1 % molybdenum, vanadium, columbiumA387/A387M9124


Chemical Composition of A691 1-1/4CR, 2-1/4CR, 5CR, 9CR, 91 Alloy STEEL PIPEs

(cast analysis, % by mass, maximum permitted unless indicated otherwise)


1CR1-1/4CR2-1/4 CR5 CR9 CR91
C0.05-0.170.05-0.170.05-0.15  0.15  0.150.08-0.12 
Mn0.40-0.65 0.40-0.650.30-0.60 0.30-0.60 0.30-0.60 0.30-0.60 
P0.025 0.0250.0250.025 0.025 0.020 
S0.025 0.025 0.025 0.025 0.025 0.010 
Si0.15-0.40 0.50-0.800.500.501.00 0.20-0.50 
Cr0.80-1.15 1.00-1.50 2.00-2.504.00-6.008.00-10.00 8.00-9.50
Mo0.45-0.60 0.45-0.650.90-1.100.45-0.650.90-1.100.85-1.05 
V  – –––0.04 0.18-0.25


*Grade 91 also includes restrictions on Nickel 0.40 max, Columbium 0.06-0.10, Nitrogen 0.030-0.070, Aluminium 0.02 max, titanium 0.01 max, Zirconium 0.01 max.


Tensile Requirements of A691 1-1/4CR, 2-1/4CR, 5CR, 9CR, 91 Alloy STEEL PIPEs

Class 1 Plates

GradeTensile (MPa)Yield (MPa)Elong. (50mm)Reduc’n of Area*
1CR380 – 550230 min22% min–
1-1/4CR415 – 585240 min22% min–
2-1/4CR, 5CR, 9CR415 – 585205 min18% min40% min
91415 – 585205 min18% min40% min

* Measured on a flat specimen

Grade                   Tensile (MPa) Yield (MPa) Elong. (50 mm) Reduc’n of Area*







2485 – 620310 min           22% min–
1-1/4CR515 – 690310 min          22% min –
1CR450 – 585275 min          22% min–
2-1/4CR, 5CR, 9CR515 – 690310 min           18% min    40% min
91585 – 760415 min           18% min–

Cangzhou Galaxy Company can arrange produce EFW or LSAW pipe for  ASTM A691 in Grade 1CR Grade-12, 1.1/4CR Grade-11, 2.1/4CR Grade-22, 3CR Grade-21, 5CR Grade-5, 9CR Grade-9, Grade-91

In addition, We prefer to supply you alloy seamless pipes, the standard is ASTM A335.


Hot Tags:

astm a106 b seamless pipe, astm a335 p22 alloy seamless pipe, SSAW pipes diameter 711mm, structure seamless pipe, astm a671 gr lsaw welded pipes

Recent Reviews
+