Chemical Composition
AISI 4130
| C | Si | Mn | P | S | Cr | Mo | Fe | |
|---|---|---|---|---|---|---|---|---|
| Min | 0.28 | 0.15 | 0.40 | • | • | 0.80 | 0.15 | 0.00 |
| Max | 0.33 | 0.35 | 0.60 | 0.040 | 0.040 | 1.10 | 0.25 | 0.00 |
AISI 4140
| C | Si | Mn | P | S | Cr | Mo | Fe | |
|---|---|---|---|---|---|---|---|---|
| Min | 0.38 | 0.15 | 0.75 | • | • | 0.80 | 0.15 | 0.00 |
| Max | 0.43 | 0.35 | 1.00 | 0.040 | 0.040 | 1.10 | 0.25 | 0.00 |
AISI 4145
| C | Si | Mn | P | S | Cr | Mo | Fe | |
|---|---|---|---|---|---|---|---|---|
| Min | 0.43 | 0.15 | 0.75 | • | • | 0.80 | 0.15 | 0.00 |
| Max | 0.48 | 0.35 | 1.00 | 0.040 | 0.040 | 1.10 | 0.25 | 0.00 |
Mechanical properties
Condition: Hardened and Tempered to 22 HRC max.
| U.T.S | 100 KSI Min | (689 N/mm2) |
|---|---|---|
| 0.2% Proof Stress | 80 KSI Min | (551 N/mm2) |
| Elongation | 20 % | |
| Red of Area | 40 % |
Condition: Hardened and Tempered to 30-36 HRC
U.T.S | 130 KSI Min | (896 N/mm2) |
|---|---|---|
| 0.2% Proof Stress | 110 KSI Min | (758 N/mm2) |
| Elongation | 13 % | |
| Red of Area | 30 % |
We offer the most complete range of standard mechanical tubing sizes available and are ready to work with you to develop custom steel tubing applications. We can create mechanical tubing solutions that offer better zinc coatings, decreased weight, longer-term corrosion resistance on interiors, and various tube strength options all handled in our factory under the careful supervision of experienced professionals.
Galaxy Company Hot Sale Seamless Steel Pipe Products:
seamless steel pipe, line pipe, ASTM A106 pipe, , Mechanical pipe, API 5L pipe, boiler tube,ASTM A335 alloy pipes,GB/T5310 boiler Tube