CGPCO

4 / 5

Q355C Material Seamless Structure Pipe Diameter 219mmx 12mm

stars, based on 0reviews
7items available

Q355 Steel Introduction

Q355 steel is a new Chinese steel grade of Low Alloy High Strength Structural Steel, which replaced Q345, the material density is 7.85 g/cm3. According to GB/T 1591 -2018, Q355 has 3 quality levels: Q355B, Q355C and Q355D. “Q” is the first letter of Chinese Pinyin: “qu fu dian”, which means Yield Strength, “355” is the minimum value of yield strength 355 MPa for steel thickness ≤16mm, and tensile strength is 470-630 Mpa.


Q355 Steel Chemical Composition (Hot Rolled)

Steel GradeQuality GradeC % (≤)Si % (≤)Mn (≤)P (≤)S (≤)Cr (≤)Ni (≤)Cu (≤)N (≤)Mo (≤)B (≤)Nb (≤)V (≤)Ti (≤)
Q355Q355B0.240.551.60.0350.0350.300.300.400.012–––––
Q355C0.200.0300.0300.012










Q355D0.200.0250.025–










Q355 Mechanical Properties (Hot Rolled)



Thickness or Dia. (d) mm; Yield Strength (≥N/mm2)







Steel GradeQuality Leveld≤1616< d ≤4040 < d ≤6363 < d ≤ 8080 < d ≤ 100100 < d ≤ 150150 < d ≤ 200200 < d ≤ 250250 < d ≤ 400
Q355Q355B355345335325315295285275–
Q355C–








Q355D265








Charpy Impact

Charpy (V-notch) impact test temperature and impact absorption energy (KV2/J).

QualityTemperatureLongitudinal Impact Energy (J), ≥Transverse Impact Energy (J), ≥
Q355B20 ℃3427
Q355C0 ℃3427
Q355D-20 ℃34 (for thickness ≥250mm)27 (for thickness ≥250mm)


Q355 Steel Equivalent Grade (Reference)

ChinaISOEN


StandardGradeStandardGradeStandardGrade
GB/T 1591 -2018Q355BISO 630-2S355BEN 10025-2 :2004S355, S355JR
Q355CS355CS355J0


Q355DS355DS355J2



A seamless pipe, as the name suggests, is a pipe without a seam or a weld-joint. Seamless pipes are thought to be able to withstand higher pressure, higher temperatures, higher mechanical stress and a corrosive atmosphere. It can be found in a wide range of applications such as in oil and gas, refinery, petrochemical, chemical, fertilizer, power, automotive, bearing, mechanical and structural.

The production of our seamless steel pipes is tightly regulated and all of the pipes we stock have been fully tested to international standards to ensure we only supply the highest quality products.


My company hot sale seamless steel line pipes:

 ASTM A106 B seamless pipes, API 5L GR.B seamless steel pipes(1” to 24” sch40, sch80),

API 5L X52, X65, X70 PSL2 seamless line pipe

Recent Reviews
+