CGPCO

4 / 5

S355JR SSAW Welded pipe 44"x 25.4mm 18m Length.

stars, based on 0reviews
7items available

Steel Grade : S355JR

Nearest Equivalent: BS4360 Gr50B; BS4360 Grade50D; BS4360 Gr50DD; DIN 17100 ST52-3; ASTM A572-50;JIS G3106 SM490; JIS 3101 SS490; ABS EH36; LRS EH36

S355 – an useful structural grade steel with a minimum yield strength of 355 N/mm².

S355 being widely used in the structural engineering and important sourceconstruction industries, S355 offers high yield and tensile strength and is supplied with a  variety of treatments and test options to ensure that it is a highly usable steel in your various projects.

S355 structural grade (S) carries minimum yield strength of 355 N/mm²m, the JR designation confirms that the link for yousteel has undergone longitudinal Chary V-Notch  impact testing at 27J (Joules) at room temperature. Other Charpy designations include J0, J2 and K2.

S    symbol for Structural Steel

JR    symbol 20 temperature impact test

J0    syambol 0 temperature impact test

J2    symbol -20 temperature impact test

EN 10219 S355 Carbon Steel Pipe

With respect to our massive knowledge and huge understanding of this pipes, we are engaged in providing Carbon Steel S355JOH EN 10219  welded pipes and seamless tubes. We are as well one of the well-known stockiest of Carbon Steel EN 10219 S355JOH Seamless Tubes, which are being used in a number of industrial functions.

Standard No:EN 10219
Outside Diameter:21.3—1800mm
Wall Thickness:1.8—-25.4mm
Length:6000 – 12 000/18 000 mm
Grade:S355JOH/S355J2H

EN 10219 S355 Carbon Steel Pipes Chemical Composition :

Steel Grade

Type of de­oxidation a

% by
mass, maximum

Steel Name

Steel Number

C

 Si

Mn

P

S

N b

S355J0H

1.0547

FF

0,22

0,55

1,60

0,035

 0,035

 0,009

S355J2H

1.0576

FF

0,22

0,55

1,60

0,030

0,030

—

S355 EN 10219  Carbon Steel Pipes Mechanical Properties :

Steel Grade

Minimum
yield strength ReH MPa

Tensile
strength Rm MPa

Minimum
elongation A d %

Minimum
impact energy KV e J

Specified thickness mm

Specified
thickness mm

Specified
thickness mm

at
test temperature of

Steel Name

Steel Number

≤
16

> 16
≤ 40

<
3

≥ 3 ≤ 40

≤ 40

-20°C

0°C

20°C

S355J0H a

1.0547

355

345

510-680

470-630

20 c

–

27

–

S355J2H

1.0576

27

–

–

S355JR steel plate min thickness 3mm up to max 400mm

SSAW welded pile can be manufactured in large lengths and diameters. Spiral welded tubular pipes are produced from internally and externally welded steel coils. Piling pipes can be welded with pipe shoes to enhance drivability in difficult ground conditions. SSAW are often coated for use in ports, bulkheads and jettys.

 

Galaxy Company Hot Sale welded Steel Pipe Products:

SSAW pipes, LSAW pipes, welded steel pipe, Galvanized pipe.

steel pipe inventory,  Chinese pipe factory, API 5L GR.B, X52 welded pipe

Recent Reviews
+