SSAW Welded linePipe API 5L X70 PSL2 42" X15.88mm 12M 3PE coating

stars, based on 0reviews
7items available

Spiral welded steel pipes are widely used in Oil, Natural Gas, Water and other flammable & nonflammable liquid conveyance and distribution pipelines, steel structures for construction and other general purposes by means of their wide size range.
Pipe Coating: HDPE/ 3PE/ 3PP/ Pipe cement mortar lining
Mill Test Certificate: EN 10204/3.1B 
Third party inspection: SGS, BV, Lloyds etc.

Chemical Analysis And Mechanical Properties Of SSAW Pipe

StandardGradeChemical Composition(max)%Mechanical Properties(min)
CSiMnPSTensile Strength(Mpa)Yield Strength(Mpa)
API 5L PSL1A0.22–0.900.0300.030335335
B0.26–1.200.0300.030415415
X420.26–1.300.0300.030415415
X460.26–1.400.0300.030435435
X520.26–1.400.0300.030460460
X560.26–1.400.0300.030490490
X600.26–1.400.0300.030520520
X650.26–1.450.0300.030535535
X700.26–1.650.0300.030570570
API 5L PSL2B0.220.451.200.0250.015415415
X420.220.451.300.0250.015415415
X460.220.451.400.0250.015435435
X520.220.451.400.0250.015460460
X560.220.451.400.0250.015490490
X600.120.451.600.0250.015520520
X650.120.451.600.0250.015535535
X700.120.451.700.0250.015570570
X800.120.451.850.0250.015625625
GB/T 9711.1L210––0.900.0300.030335335
L245––1.150.0300.030415415
L290––1.250.0300.030415415
L320––1.250.0300.030435435
L360––1.250.0300.030460460
L390––1.350.0300.030490490
L4150.26–1.350.0300.030520520
L4500.26–1.400.0300.030535535
L4850.23–1.600.0300.030570570
GB/T3091/ SY/T503Q1950.120.300.500.0350.040315315
Q215B0.150.351.200.0450.045335335
Q235B0.200.351.400.0450.045370370
Q345B0.200.501.700.0350.035470470
ASTM A53A0.250.100.950.0500.045330330
B0.300.101.200.0500.045415415
ASTM A2521–––0.050–345345
2–––0.050–414414
3–––0.050–455455
EN10217-1P195TR10.130.350.700.0250.020320320
P195TR20.130.350.700.0250.020320320
P235TR10.160.351.200.0250.020360360
P235TR20.160.351.200.0250.020360360
P265TR10.200.401.400.0250.020410410
P265TR20.200.401.400.0250.020410410
EN10217-2P195GH0.130.350.700.0250.020320320
P235GH0.160.351.200.0250.020360360
P265GH0.200.401.400.0250.020410410
EN10217-5P235GH0.160.351.200.0250.020360360
P265GH0.200.401.400.0250.020410410
EN10219-1S235JRH0.17–1.400.0400.040360360
S275JOH0.20–1.500.0350.035410410
S275J2H0.20–1.500.0300.030410410
S355JOH0.220.551.600.0350.035470470
S355J2H0.220.551.600.0300.030470470
S355K2H0.220.551.600.0300.030470470