CGPCO

4 / 5

SUS 316Ti Stainless Steel Seamless Pipe 12in SCH80

stars, based on 0reviews
7items available

316Ti STAINLESS STEEL PIPE BRIEF INTRODUCTION

316Ti stainless steel pipe is a hollow long round steel pipe which is widely used in petroleum, chemical, medical, food, light industry, machinery, instrument and other industrial pipeline and mechanical structure parts, etc. In addition with in bending and torsion strength, the weight is lighter, so it is also widely used to make mechanical parts and engineering structures. It is also used to produce all kinds of conventional weapons, guns and shells.

Chemical Composition of ASTM A312 / A213 SS TP316Ti Pipe and Tube
GradeCMnSiPSCrMoNiFe
SS TP 316Ti0.08 max2.0 max0.75 max0.045 max0.030 max16.00 – 18.002.00 – 3.0010.00 – 14.0068.395 min

Mechanical Property of Stainless Steel UNS S31635 Pipes and Tubing
DensityMelting PointTensile StrengthYield Strength (0.2%Offset)Elongation
8.0 g/cm31399 °C (2550 °F)Psi – 75000 , MPa – 515Psi – 30000 , MPa – 20535 %

316Ti Stainless Steel Pipes and Tubing Equivalent Grades
GradeNorth AmericaFranceGermanyEuropeanJapanRussiaEuropeanItalySwedenUKUSA
UNSAFNORDINW.N.JISGOSTENUNISISBSAISI
SS 316TiS31635Z 2 CND 17-13-AzX 5 CrNiMo 17 13 31.4571–08KH16N13M2BX 3 CrNiMo 17 13 3X 2 CrNiMo 171323 53316S13316Ti


Size (Seamless) : 1/2″ NB – 16″ NB

Size (ERW) : 1/2″ NB – 24″ NB

Size (EFW) : 6″ NB – 100″ NB

Outside Diameter : 6.00 mm OD up to 914.4 mm OD, Sizes up to 24” NB available Ex-stock, OD Size Steel Tubes available Ex-stock

Thickness Range : 0.3mm – 80 mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS

Length : Single Random, Double Random & Required Length End: Plain End, Beveled End, Treaded

Type : Seamless, ERW, Welded, Fabricated, CDW

Form : SS 316Ti Round Pipes/Tubes, SS 316Ti Square Pipes/Tubes, SS 316Ti Rectangular Pipe/Tubes, SS 316Ti Coiled Tubes, SS 316Ti “U” Shape, SS 316Ti Pan Cake Coils, SS 316Ti Hydraulic Tubes

Inspection, Test Reports : Mill Test Certificates, EN 10204 3.1, Chemical Reports, Mechanical Reports, PMI Test Reports, Visual Inspection Reports, Third Party Inspection Reports, NABL Approved Lab Reports, Destructive Test Report, Non Destructive Test Reports

Delivery Condition : Annealed and Pickled, Polished, Bright Annealed, Cold Drawn

 Galaxy Company Hot Sale stainless Steel Pipe Products:

 TP304/304L, TP316/TP316L, S31803, TP347H,stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80)

Recent Reviews
+