ASTM A335 alloy steel pipes fit ASTM A234 WPx series buttweld fittings (WP5, WP9, WP91) and A182 Fx forged fittings and flanges (A182 F5, F9, F11, F22, F91). All these materials have similar chemical and mechanical properties and can be joined or welded.

CHEMICAL COMPOSITION

The types of alloy steel pipes covered by the ASTM A335 – ASME SA335 specification are designed with a “P” prefix, from P5 to P92. Grades P11/P22 and P91/92 are typically found in power stations, whereas grade P5 and P9 are more common for application in the petrochemical industry. Grades P9, P91 are, in the list, the more expensive.

ASTM A335
Low-Alloy Steel
(Grades)
UNS
equivalent
C≤MnP≤S≤Si≤CrMo
P1K115220.10~0.200.30~0.800.0250.0250.10~0.50–0.44~0.65
P2K115470.10~0.200.30~0.610.0250.0250.10~0.300.50~0.810.44~0.65
P5K415450.150.30~0.600.0250.0250.54.00~6.000.44~0.65
P5bK515450.150.30~0.600.0250.0251.00~2.004.00~6.000.44~0.65
P5cK412450.120.30~0.600.0250.0250.54.00~6.000.44~0.65
P9S504000.150.30~0.600.0250.0250.50~1.008.00~10.000.44~0.65
P11K115970.05~0.150.30~0.610.0250.0250.50~1.001.00~1.500.44~0.65
P12K115620.05~0.150.30~0.600.0250.0250.50.80~1.250.44~0.65
P15K115780.05~0.150.30~0.600.0250.0251.15~1.65–0.44~0.65
P21K315450.05~0.150.30~0.600.0250.0250.52.65~3.350.80~1.60
P22K215900.05~0.150.30~0.600.0250.0250.51.90~2.600.87~1.13
P91K915600.08~0.120.30~0.600.020.010.20~0.508.00~9.500.85~1.05
P92K924600.07~0.130.30~0.600.020.010.58.50~9.500.30~0.60

MECHANICAL PROPERTIES

Hardness
A335 Low-Alloy PipeUNS NumberYield Strength ksiTensile Strength ksiElongation %RockwellBrinell
P1K11522305530––
P2K11547305530––
P5K41545407030–207 max
P9S50400306030––
P11K11597306020––
P12K11562326030–174 max
P22K21590306030––
P91K91560608520––


Hot Tags:

Seamless boiler tube, seamless pipe 42CrMo, aviation fuel transmission seamless pipe, ssaw welded pipe for oil conveying, ssaw pile pipe astm a252, carbon steel seamless pipe sour service, ssaw welded pipe x52