CGPCO

4 / 5

Seamless Pipe ASTM A106 C 508mmX22.23mm 6 M Length

stars, based on 0reviews
7items available

ASTM A106 pipe is the carbon seamless steel pipe that widely used for different industries. For oil and gas pipelines, water transmissions, mineral slurry, boiler and high pressure services, construction and structural.

A106 pipe has three grades: Grade A and Grade B and C, where in most circumstances used for Grade B.


Mechanical Properties – Tensile Requirements

 Grade AGrade BGrade C
Tensile Strength, min, psi48,00060,00070,000
Yield Strength, min, psi30,00035,00040,000

Chemical Requirements

ElementGrade AGrade BGrade C
Carbon max. %0.250.300.35
Manganese %0.27 – 0.93 0.29 – 1.06 0.29 – 1.06 
Phosphorus max %  0.0350.0350.035
Sulfur max %0.0350.0350.035
Silicon, min %0.100.100.10


Standard: ASTM A106, ASME SA106 (NACE MR0175 also applicable for H2S environment).

Grade: A, B, C
Outer diameter: 1/2”, 1”, 2”, 3”, 4”, 6”, 8”, 10”, 12” up to NPS 24 inch
Wall thickness: SCH 10, SCH 20, SCH STD, SCH 40, SCH 80, to SCH160, SCHXX

Range of length: Single Random Length or Double Random Length. Fixed Length 6 meter or 12 meters.
Ends type: Plain end, Beveled, Threaded
Coating: Black paint, Varnished, Epoxy Coating, Polyethylene Coating, FBE, 3PE, CRA Clad and Lined.


Seamless Pipe ASTM A106 C 508mmX22.23mm 6 M Length

Seamless Pipe ASTM A106 C 508mmX22.23mm 6 M Length

Seamless Pipe ASTM A106 C 508mmX22.23mm 6 M Length


Seamless Pipe ASTM A106 C 508mmX22.23mm 6 M Length



Hot Tags: seamless pipe astm a106 c 508mmx22.23mm 6 m length, China, suppliers, factory, cheap, price, discount, bulk, customized, seamless pipe in large caliber, carbon steel seamless pipe sour service, seamless pipe en10305, astm a519 seamless mechanical tube, astm a312 tp347h stainless steel tube for heat exchanger, erw pipe api 5l x60

Recent Reviews
+