ASTM A106 / A106M Standard Specification For Seamless Carbon Steel Pipe For High-Temperature Service

Carbon Steel Pipe ASTM A 106 Gr C pipes are used in the construction of petrochemical plants, power plants, oil and gas refineries, boilers and ships wherein fluids are transported.

Sizes: 1/8″ NB – 30″ NB

Wall Thickness available:Schedule 20 – Schedule XXS (heavier on request) up to 250 mm thick.


SPECIFICATIONA106 NPS 1/8 — 30" ANSI Schedules to 160
SCOPECovers SEAMLESS carbon steel nominal wall pipe for high-temperature service, suitable for bending, flanging and similar forming operations.

NPS 1 1/2 and under may be either hot finished or cold drawn. NPS 2 and larger shall be hot finished unless otherwise specified.

KINDS OF STEEL PERMITTED FOR
FOR PIPE MATERIAL
Killed Steel
Open-hearth
Electric-furnace
Basic-oxygen
HOT-DIPPED
GALVANIZING
Not covered in specification.
PERMISSIBLE VARIATIONS
IN WALL THICKNESS
The minimum wall thickness at any point shall not be more than 12.5% under the nominal wall thickness specified.

ASTM A106 Grade B Pipe Chemical Compositions And Mechanical Strength