Products: API SPEC 5CT Casing Pipe and Tubing & Casing.
Types: Seamless casing and ERW casing
Applications: It is widely used for oil casing and tubing in oil wells
Grades: API 5CT J55/K55/N80/L80-1/L80-9Cr/L80-13Cr/P110/Q125/K55 D10/L80 D10.
Special Service: Sweet Service, Sour Service, Anti-H2S, NACE MR0175/ISO15156
Produce Process: Hot Rolled, Cold Drawn, Hot Expanded.
Accessories: Pup Joint, Coupling (Coupling Stock), Blast Joint, Crossover etc.
Connection: API connection and Premium connection, like TPCQ, HSM etc.

A full length non destructive inspection is performed in accordance with API 5CT for external and internal, longitudinal
and transverse defects with a standard notch depth equal to 5% of the specified wall thickness.


 

Dimension Tolerance

Types of steel tubes
Outer Diameter
Wall Thickness
Cold-rolled tubes
Tube sizes(mm)
Tolerances(mm)
Tolerances(mm)
<114.3
±0.79
-12.5%
≥114.3
-0.5%,+1%

 hemical Composition

StandardGradeChemical compositions(%)
API SPEC 5CT
J55
CSiMnPSCrNiCuMoV
K550.34~0.39
0.20~0.35
1.25~1.50
≤0.020
≤0.015
≤0.15
≤0.20
≤0.20
//
N80
0.34~0.38
0.20~0.35
1.45~1.70
≤0.020
≤0.015
≤0.15
///0.11~0.16
L80
0.15~0.22
≤1.00
0.25~1.00
≤0.020
≤0.010
12.0~14.0
≤0.20
≤0.20
//
P110
0.26~0.395
0.17~0.37
0.40~0.70
≤0.020
≤0.010
0.80~1.10
≤0.20
≤0.20
0.15~0.25
≤0.08

 


Mechanical properties

GradeTypeTotal elongation under load (%)
Yield strength (min)
Yield strength (max)
Tensile strength min Mpa
Hardness Max (HRC)
Hardness Max (HBW)
J55-0.5
379552517--
K55-0.5
379552655--
N8010.5
552758689--
N80Q0.5
552758689--
L8010.5
55265565523241
L80
9Cr0.5
55265565523241
L80
13Cr0.5
55265565523241
C90-0.5
62172468925.4255
C95-0.5
655758724--
T95-0.565575872425.4255
P110-0.6758965862--
Q125All0.658621034931--

 

Oil casing is used to support the oil, gas wells of steel pipe, in order to ensure the drilling process and the completion of the entire well after the normal operation. Each well has several layers of casing depending on the drilling depth and geology. Casing down to use cement cementing, it and the tubing, drill pipe is different, can not be reused, a one-time consumption of materials. Therefore, the casing of the total consumption of more than 70% of the wells. Casing according to the use can be divided into: catheter, surface casing, casing technology and oil casing.

 

 

Seamless Pipe Casing API 5CT L80   9 5/8"  53.5PPF   BTC R3

Seamless Pipe Casing API 5CT L80   9 5/8"  53.5PPF   BTC R3

Seamless Pipe Casing API 5CT L80   9 5/8"  53.5PPF   BTC R3

 

Hot Tags: seamless pipe casing api 5ct p110, China, suppliers, factory, cheap, price, discount, bulk, customized, seamless pipes with grooved end, erw pipes diameter 711mm, seamless pipe for sour service, seamless pipe astm a53, seamless pipe din17175, astm a671 gr lsaw welded pipes

Recent Reviews
+