CGPCO

4 / 5

Seamless Steel line Pipe API 5L X65 PSL2 14" SCH80 12 M LENGTH

stars, based on 0reviews
7items available

API 5L LINE PIPE

Specification API 5L covers seamless and welded pipe suitable for use in conveying gas, water, oil, and other liquefied media.


PSL 1

GRADE

Chemical Composition

Mechanical Property

C (Max)

Mn (Max)

P (Max)

S (Max)

TENSILE ( Min )

YIELD ( Min )

Psi X 1000

Mpa

Psi X 1000

Mpa

A25

CL   I

0.21

0.60

0.030

0.030

45

310

25

172

CL  II

0.21

0.60

0.030

0.030

A

0.22

0.90

0.030

0.030

48

331

30

207

B

0.26

1.20

0.030

0.030

60

414

35

241

X42

0.26

1.30

0.030

0.030

60

414

42

290

X46

0.26

1.40

0.030

0.030

63

434

46

317

X52

0.26

1.40

0.030

0.030

66

455

52

359

X56

0.26

1.40

0.030

0.030

71

490

56

386

X60

0.26

1.40

0.030

0.030

75

517

60

414

X65

0.26

1.45

0.030

0.030

77

531

65

448

X70

0.26

1.65

0.030

0.030

82

565

70

483


PSL 2

GRADE

Chemical Composition

Mechanical Property

C 
(Max)

Mn 
(Max)

P 
(Max)

S 
(Max)

Tensile

Yield

C. E.      IMPACT ENERGY

Psi x 1000

Mpa

Psi x 1000

Mpa

PCM

IIW

J

FT/LB

B

0.22

1.20

0.025

0.015

60 - 110

414 - 758

35 - 65

241 - 448

0.25

0.43

T/L 27/41

T/L 20/30

X42

0.22

1.30

0.025

0.015

60 - 110

414 - 758

42 - 72

290 - 496

0.25

0.43

T/L 27/41

T/L 20/30

X46

0.22

1.40

0.025

0.015

63 - 110

434 - 758

46 - 76

317 - 524

0.25

0.43

T/L 27/41

T/L 20/30

X52

0.22

1.40

0.025

0.015

66 - 110

455 - 758

52 - 77

359 - 531

0.25

0.43

T/L 27/41

T/L 20/30

X56

0.22

1.40

0.025

0.015

71 - 110

490 - 758

56 - 79

386 - 544

0.25

0.43

T/L 27/41

T/L 20/30

X60

0.22

1.40

0.025

0.015

75 - 110

517 - 758

60 - 82

414 - 565

0.25

0.43

T/L 27/41

T/L 20/30

X65

0.22

1.45

0.025

0.015

77 - 110

531 - 758

65 - 82

448 - 565

0.25

0.43

T/L 27/41

T/L 20/30

X70

0.22

1.65

0.025

0.015

82 - 110

565 - 758

70 - 82

483 - 565

0.25

0.43

T/L 27/41

T/L 20/30

X80

0.22

1.90

0.025

0.015

90 - 120

621 - 827

80 - 102

552 - 705

0.25

0.43

T/L 27/41

T/L 20/30

 


IMPACT TEST

AVG ABSORBED ENERGYIND. ABSORBED ENERGY
MIN (JOULES)MIN (JOULES)
2720

Notes:

Whether you need Carbon Steel API 5L Gr. X70 Seamless Pipe, standard length and diameter pipes and tubing or you need high strength, high tensile, heavy wall linepipe requirements for deep sour wells, drilling, offshore drilling and production, arctic exploration and production, or you need Carbon Steel API 5L Gr. X70 Seamless Pipe for natural gas, oil or water transport, then Trident Steel & Engg. Co. can meet the demands of your company.


My company hot sale steel pipe:


API 5L X65, X70 PSL2 SSAW welded pipes, (20” to 60” sch40, sch80, sch160),

API 5CT seamless casing

API 5L X52, X65, X70 PSL2 seamless line pipe (2” to 24” sch40, sch80, sch160),

Recent Reviews
+