Seamless Tubing API 5CT L80 CR13 114.3mm 12.60ppf R2
API 5CT L80 13Cr Corrosion Resistant Stainless Steel Tubing
L80-13CR Tubingis a martensitic stainless steel used in the hardened and tempered condition. manufactured to API specification 5CT. This is a controlled yield strength material with a hardness testing requirement. Used in wells with carbon dioxide environments.
Available in casing dimensions of 114.3 mm (4.5") to 339.7 mm (13.38")
Available in tubing dimensions of 60.3 mm (2.38") to 114.3 mm (4.5")
We provide 13CR L80 Chromium grades and Corrosion Resistant Alloys (CRA) for oil and gas operations in highly corrosive environments where carbon pipe cannot be used.13CrM and 13CrS have better performance with regards to corrosion resistance and excellent toughness.
In most conditions when the partial pressure of CO2 is above 30psi, carbon steels present high corrosion rates. Steel grades alloyed with high contents of Chromium (Cr), Molybdenum (Mo) and Nickel (Ni) are able to effectively resist corrosion.
13Cr-L80 seamless tubes are used for oil well serving in resistant corrosive environment, which requires excellent quality of resistant corrosion and strength, also requires high precision of bend and size.
CO2 -corrosion is one of the four main corrosion forms in oil-gas field and has become a very outstanding issue during the development of petroleum industries. Most of largest oil fields, rich in CO2 content, such as Daqing, Tarim, Changqing etc. now has been exposed to serious CO2 corrosion threat. The low alloy steel pipe we often used in the past now has faced serious corrosion condition, thus making us have to use corrosion resister. In the short run, applying corrosion resister is easy to operate and low cost, but it will lead to environmental pollution in the long run. Under this circumstance, we designed and developed the L80-13Cr anti-corrosion casing & tubing and got a very good effect.
This product is non-API products, the produce and inspection standard of which exceeds the API requirements. These products use the 13 Cr steel, the chemical composition and the manufacturing process of which are reliable.
The anti-corrosion simulation experiment has been done in Xi’an OCTG Research Center of CNPC, the result is as follows:
1.The chemical composition,grain size,inclusion,hardness and mechanical property comply with the relevant standard;
2. By evaluating the electrochemical corrosion of the submission specimen as per ASTM G3 standard, we found that the surface of the specimen is capable of passivating and healing certain passive film.
3.Under the circumstance of simulated oil-field corrosion medium(1MPa CO2,90°C), we made the evaluation test of the submission specimen and found it has good corrosion- resistance ; The average corrosion rate is 0.054mm and 0.156mm per year respectively under dynamic and static state; the surface basically render uniform corrosion and no serious spot corrosion.
Chemical Composition
| C | Mn | Mo | Cr | Ni | Cu | Ti | P | S | Si | V | Al | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Min | 0.150 | 0.250 | - | 12.000 | - | - | - | - | - | - | - | - |
| Max | 0.220 | 1.000 | - | 14.000 | 0.500 | 0.250 | - | 0.020 | 0.010 | 1.000 | - | - |
Mechanical Propertie
| Tensile Strength | 655 MPa min | 95,000 psi min |
| Yield Strength | 552 MPa min | 655 MPa max |
| 80,000 psi min | 95,000 psi max | |
| Total Elongation Under Load | 0.500 % | - |
| Hardness | 23 Max HRC | 241 Max HBW |
Our Services/Warranty
Available in casing dimensions of 114.3 mm (4.5") to 339.7 mm (13.38")
Available in tubing dimensions of 60.3 mm (2.38") to 114.3 mm (4.5")
As a professional manufacturer, we provide follow services:
1.Lower price
2.ONE year warranty and life time maintenance
3.In time delivery.
4.High Quality assurance..
Galaxy company hot sale steel pipe and pipe fittings:
API 5CT seamless casing, and tubing, (2 3/8” to 20” K55, J55, N80, L80, P110),