Chemical Composition (%, max) | ||||||||
Steel Grade | C | Si | Mn | Cr | Ni | Mo | S | P |
TP304 | 0,08 | 0,75 | 2 | 18 - 20 | 8 - 11 | - | 0,03 | 0,04 |
TP304L | 0,035 | 0,75 | 2 | 18 - 20 | 8 - 13 | - | 0,03 | 0,04 |
TP316 | 0,08 | 0,75 | 2 | 16 - 18 | 11 - 14 | 2 - 3 | 0,03 | 0,04 |
TP316L | 0,035 | 0,75 | 2 | 16 - 18 | 10 - 15 | 2 - 3 | 0,03 | 0,04 |
TP321 | 0,08 | 0,75 | 2 | 17 - 20 | 9 - 13 | - | 0,03 | 0,04 |
Mechanical properties
| |||
Steel Grade | Tensile Strength, N/mm2 (min) | Yield Strength, N/mm2 (min) | Elongation, % (min) |
TP304 | 515 | 205 | 35 |
TP304L | 485 | 170 | 35 |
TP316 | 515 | 205 | 35 |
TP316L | 485 | 170 | 35 |
TP321 | OD < 17,1 mm - 515; | OD < 17,1 mm - 205; | 35 |
ASTM A213 TP 304L stainless pipe
TP304L Stainless Steel Pipe is widely used in petroleum, chemical, medical, food, light industry, machinery, instrument and other industrial pipeline and mechanical structure parts, etc. In addition, in bending and torsion strength, the weight is lighter, so it is also widely used to make mechanical parts and engineering structures.
My company hot sale stainless steel pipe:
TP304/304L, TP316/TP316L, stainless steel welded and seamless pipes, (1” to 48” sch10, sch20, sch40, sch80),