CGPCO

4 / 5

Stainless Steel welded Tube ASTM A213 TP304L 12in Diameter SCH10S 12M Length

stars, based on 0reviews
7items available

ASTM A312 covers seamless and straight-seam welded austenitic pipe intended for high temperature and general corrosive service. Stainless steel pipe ASTM A312 has 4 main grades TP304/304L, TP316/316L. TP304/TP304L and TP347 are included in ASME pressure vessel code and the Chemical Plant and Refinery Piping Code, These steel tubes are safe to be used in temperatures as low as −425 °F [−250 °C] without impact tests qualification.


ASTM A312 Chemical Composition:

Steel GradeASTM A312  Chemical Composition % Max
CMnPSSiCrNiMoN BNbTi
TP3040.082.000.0450.0301.0018.0-20.08.0-11.0……… .…
TP304H0.04-0.102.000.0450.0301.0018.0-20.08.0-11.0…………
TP304L0.035 D2.000.0450.0301.0018.0-20.08.0-13.0…………
TP310S0.082.000.0450.0301.0024.0-26.019.0-22.00.75


TP3160.082.000.0450.0301.0016.0-18.011.0-14.02.00-3.00………
TP316L0.0352.000.0450.0301.0016.0-18.010.0-14.02.00-3.00………
TP316H0.04-0.102.000.0450.0301.0016.0-18.011.0-14.02.00-3.00………
TP316Ti0.082.000.0450.0300.7516.0-18.010.0-14.02.00-3.000.10…5x(C+N)-0.70
TP3210.082.000.0450.0301.0017.0-19.09.0-12.0…0.10…5C-0.70
TP321H0.04-0.102.000.0450.0301.0017.0-19.09.0-12.0………4C-0.60
TP3470.082.000.0450.0301.0017.0-19.09.0-13.0

10xC-1.00…
TP347H0.04-0.102.000.0450.0301.0017.0-19.09.0-13.0……8xC-1.00…

ASTM A312 Mechanical Property:

ASTM A312  Mechanical Properties
Steel GradeHeat
Treatment
Temperure
Min.
º F(º C)
Tensile Strength
Ksi (MPa), Min.
Yield Strength
Ksi (MPa), Min.
Elongation %, Min
TP304Solution1900 (1040)75(515)30(205)35
TP304LSolution1900 (1040)70(485)25(170)35
TP304HSolution1900 (1040)75(515)30(205)35
TP310SSolution1900 (1040)75(515)30(205)35
TP316Solution1900(1040)75(515)30(205)35
TP316LSolution1900(1040)70(485)25(170)35
TP316HSolution1900(1040)75(515)30(205)35
TP316TiSolution1900(1040)75(515)30(205)35
TP321Solution1900(1040)75(515)30(205)35
TP321HSolutionCold: 2000(1100)
Hot: 1925(1050)
75(515)30(205)35
TP347Solution1900(1040)75(515)30(205)35
TP347HSolutionCold: 2000(1100)
Hot: 1925(1050)
75(515)30(205)

ASTM A312 Equivalent Steel Grade:

ASTM A312JIS G3459DIN 17440BSNF
TP304SUS 304 TPX5CrNi 18 9304S18A 49-230
TP304HSUS 304 HTP
304S59A 49-214
TP310304 LTPX2 CrNi 19 9304S14A 49-230
TP316SUS 304L TP


TP316H310STPX5 CrNiMo 18 10316S18A 35-573
TP316LSUS 316 TP
316S59A 49-230
TP321SUS 316 LTPX2 CrNiMo 18 10316S14A 49-230
TP347316 HTPx10 CrNiTi 18 9321S18A 49-230
TP347HSUS 316 LTPX5 CrNiNb 18 9347S18A 35-573

Cangzhou Galaxy Steel Pipe can supply ASTM A312 stainless steel tube from stock or from production. If you are interested in buying ASTM A312 steel tube products, contact us for the latest price.


Stainless tube Specifiaction

  • OD: 10.3mm-609.6mm

  • WT: 0.2mm-60mm

  • Length: 5-12m

  • Application: Low pressure line pipe for liquid, water, gas, oil, pipe for boiler project, etc.

  • Supplementary Technology: Plain or threaded with socket or beveled with plastic caps, hydraulic testing, eddy current, Infrared test.

  • Surface: Bright annealed, pickled, blasted or passivated.

  • Delivery State: Hot Rolled, Cold Drawn, ERW welded


Galaxy Company Hot Sale stainless Steel Pipe Products:

TP304/304L, TP316/TP316L, S31803, TP347H,stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80),

Recent Reviews
+