alloy steel
A Brief Description Of Microalloy Steel
View: 104
The role of microalloy elements in steel is to refine grains in order to improve the strength and toughness of steel, while relying on the analysis of microalloy elements to further improve the strength. The commonly used microalloy elements in steel are Ti, Nb, V and Al, their role in steel is generally by precipitating reinforcement to improve the strength of steel, the solid-dissolved reinforcement effect on the strength of steel contribution is much lower.
Relative to the low-carbon content of flat material, medium-carbon special steel often contains a high nitrogen content, so that in the steel will inevitably form a large size TiN, these large-size TiN precipitate and steel in the solidification process produced by the first precipitate material fatigue and toughness is very harmful, so to limit the upper limit of micro-alloying elements. For steels containing Cr and Mo, when the Nb content is 0.09% and the carbon content is more than 0.6%, even under equilibrium conditions there will still be a precipitate. Before forging the material, a higher heating and insulation temperature is usually used to allow the Nb carbide and carbon nitride formed by the steel water to be fully soluble during the continuous casting process. For wrought steels of 0.5% C and 0.06% Nb, Nb compounds will not be fully soluble at a conventional heating temperature of 1250 degrees C. When the lower the carbon content in the steel, the higher the amount of Nb that dissolves at the same temperature.
The solubility of microalloy elements in steel is not only affected by carbon content, but also by nitrogen content, but has little effect on the solubility of microalloyed elements in high-carbon steel. For steel spallatium sprees with relatively high alloy element content, the partial analysis of alloy elements needs to be considered, especially when the use of die casting to produce raw materials, because the internal solidification rate of the ingots is very low, more likely to lead to macro-bias generation. The results show that the degree of polarization of Nb increases with the increase of carbon content in steel, which is the maximum when the carbon content is 0.2%-0.5%. According to the empirical formula provided in the literature, the carbon content in steel also changes the spacing of secondary branches and has a minimum value at 0.15% C. In addition to the carbon content, the bias coefficient of Nb in steel is also affected by other alloying elements, and si and Mo, which promote the formation of ferrite, reduce s, while N and Ni increase the polarization trend of Nb.
0users like this.