Heat-resistant steel refers to the special steel with higher strength and good chemical stability at high temperature. It includes oxidation resistant steel (high temperature non - peeling steel) and thermal strength steel two categories. Oxidation resistant steel is usually used in the temperature range of 550 ~ 1250℃, requiring better chemical stability (such as oxidation resistance and high temperature corrosion resistance, etc.), but the load is low, and the resistance to creep and creep fracture is not high. Thermal strength steel is usually used in the temperature range of 450 ~ 900℃. It bears large stress and requires the material to have good creep resistance, break resistance and oxidation resistance.


Heat resistant steel is widely used. The main equipment components of boilers, steam turbines and gas turbines in thermal power plants are made of heat-resistant steel. In the petrochemical industry, the key equipment of refinery, ammonia and ethylene plant can not do without heat-resistant steel. In addition, it is widely used in metallurgy, machinery, building materials, light industry and other industrial furnaces as heat-resistant structural materials. In coal liquefaction, gasification and nuclear energy (such as high temperature gas cooled reactor, fast reactor) some core structural materials also use a large number of heat resistant steel.


Due to the development of power station and petrochemical industry, molybdenum was found to be an effective element to improve the thermal strength of heat-resistant steel in the 1930s. Adding 0.5% molybdenum to mild steel can increase the working temperature from 450℃ to 500℃. In order to solve the problem of the graphitization of molybdenum steel, low-alloy chromium-molybdenum steel was developed. In 1938, steel containing 0.8% chromium and 0.5% molybdenum (equivalent to 15CrMo) was used in boiler superheater in Britain. Later, steels with higher performance such as 10.25chromium-0.5Molybdenum and 2.25chromium-1 molybdenum were developed. In order to further improve the thermal strength of steel and save molybdenum resources, a series of chromium-molybdenum-vanadium steel was developed. 12CrlMoV of the former Soviet Union is a typical representative, which is still the main material for manufacturing power plant boilers.

Medium and high alloy heat resistant steel is basically and stainless steel developed at the same time, in 1914 Germany Strauss et al pointed out that steel containing enough nickel and chromium has oxidation resistance and acid resistance, after 1920 gradually developed chromium and chromium nickel stainless heat resistant steel, and formed a variety of branches. For example, the blade steel series is mainly used for steam turbine and gas turbine blades. Valve steels for intake and exhaust valves of internal combustion engines in automobiles and tractors, including chromium-silicon, chromium-nickel and chromium-manganese nickel-nitrogen shaped steels; Used in metallurgical machinery, petrochemical, light industry, building materials industrial furnace heat resistant steel and heat resistant cast steel, including high chromium ferritic steel and high chromium nickel austenitic steel. Because heat resistant cast steel has higher creep strength than deformation material, it has been widely used in petrochemical and furnace materials in recent 20 years. A series of high chromium nickel austenitic heat resistant cast steel reinforced with tungsten, molybdenum, niobium, titanium and so on has been developed. Widely used in ammonia and ethylene cracking units. In the field of heat-resistant steel, the world's developed countries use more mature, has formed their own special standards.

Role of alloying elements (1) Chromium, aluminum, silicon. These elements form and stabilize ferrite and can promote the formation of dense oxide film on the surface of steel at high temperature to prevent further oxidation, which is the main element to improve the oxidation resistance of steel and high temperature gas corrosion resistance. However, the high content of aluminum and silicon in steel will seriously deteriorate the plasticity and thermoplasticity at room temperature. Chromium can significantly increase the recrystallization temperature of low alloy steel, and when the content is 2%, the strengthening effect is the best. (2) Nickel, manganese. It can form and stabilize austenite. Improve the high temperature strength and carburizing resistance of austenitic steel. Manganese can replace nickel to form austenite, but it will impair the oxidation resistance of heat resistant steel. (3) Molybdenum and tungsten. It's a ferrite forming element. It can increase the recrystallization temperature of steel and increase the creep strength of heat-resistant steel mainly by solution strengthening. Molybdenum is the most important element to improve the thermal strength in low alloy steel, and the combination of tungsten and molybdenum has more obvious effect than the single addition. Because molybdenum and tungsten are easy to volatilize and oxidize at high temperature, excessive addition of molybdenum and tungsten to steel will adversely affect the oxidation resistance at high temperature. (4) Vanadium, niobium, titanium. It is a ferrite forming element and a strong carbide forming element, which can form fine and dispersed carbides and improve the high temperature strength of steel. The combination of titanium, niobium and carbon can also prevent intergranular corrosion of austenitic steel at high temperature or after welding. (5) carbon and nitrogen. It can enlarge and stabilize the austenite, so as to improve the high temperature strength of heat-resistant steel. When the steel contains more chromium and manganese, it can significantly improve the melting degree of nitrogen. Adding nitrogen or increasing the content  of carbon can replace the precious metal nickel. The formation of carbides or carbonitrides and control of their form and quantity can further strengthen the system. (6) Boron and rare earth. Are trace elements in heat resistant steel. When boron is dissolved into the solid solution, the crystal lattice will be distorted, and boron on the grain boundary can prevent element diffusion and grain boundary migration, thus improving the high temperature strength of steel. Adding trace rare earth into steel can improve the oxidation resistance and thermoplasticity of steel. The enrichment of rare earth in grain boundaries can purify and strengthen grain boundaries, which is beneficial to improve the thermal strength of steel. But add rare earth type, quantity and %26lsquo; The addition method is very important, the existence state of rare earth in steel should be properly controlled, otherwise it is difficult to get the desired effect.

Classification of heat resistant steel according to its organization can be divided into 4 classes, pearlite heat resistant steel, martensitic heat resistant steel, ferritic heat resistant steel and austenitic heat resistant steel.


Brief Introduction Of Heat-Resistant Steel

Brief Introduction Of Heat-Resistant SteelBrief Introduction Of Heat-Resistant Steel

My company hot sale steel pipe

Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),

ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),

TP304/304L, TP316/TP316L, stainless steel pipes, (1” to 48” sch10, sch20, sch40, sch80),

 

0users like this.

Leave a Reply

RSS

Get in touch

Refresh Code