Effect of heat treatment on persistent creep properties of superalloys


The most basic heat treatment of superalloys is solution and aging. Solution treatment temperature can make γ´ phase and carbide solution, grain growth, and obtain high durable strength. Low solution temperature can not dissolve high temperature carbides, only the main enhanced phase grain is small, can obtain high instantaneous tensile strength. Medium solution treatment temperature can obtain better comprehensive properties, the aging of superalloy can be adopted single stage or multistage mode, the aging temperature should be slightly higher than the service temperature, so that the alloy can obtain more stable microstructure state.


The key factors determining the microstructure and properties of fe-base superalloy are solution treatment temperature and holding time, and cooling method has little influence. With the increase of solution temperature, the tensile strength of the alloy decreases and the ductility increases below 550℃. However, the high temperature strength is almost unchanged, and the high temperature plasticity decreases. The durable strength increases with the increase of solution temperature, reaches the peak value at a certain temperature (such as 1150℃~1170℃), and then decreases. The persistent plasticity tends to decrease with the increase of solution temperature. The purpose of aging treatment is to obtain the second phase with reasonable quantity, morphology and distribution. For the aging hardening alloy, the aging process is accelerated with the increase of aging temperature, and the maximum hardness of the alloy increases. When the temperature exceeds a certain level, the maximum hardness of aging decreases.


During the aging process, the carbides precipitate at grain boundary and ingrain boundary, forming M23C6 or M6C carbides in autumn or chain form at grain boundary, which can change the durable creep property of the alloy, while the formation of membrane or cell carbides will reduce the durable plasticity of the alloy and cause the persistent notch sensitivity. Some γ´ phase reinforced superalloys are commonly used in the secondary aging or step aging process, so that two different sizes of γ´ phase particles can be obtained, so that the alloy can obtain better comprehensive properties.


When the yield strength and creep strength of some alloys are still low after two aging treatments, the first aging temperature can be increased and the third aging can be increased.


Nickel base and iron base superalloys have the same matrix and similar type of the second phase, so the heat treatment principle and process of the two kinds of alloys are the same. Nickel base superalloys include solution strengthening and precipitation strengthening. In the process of forming, they often need intermediate annealing and stress relief annealing; But the heat treatment process which mainly determines its properties is solution treatment or solution + aging treatment.



The key of the heat treatment process of nickel-base superalloy is to choose the solution treatment temperature reasonably according to the service conditions of the workpiece. The grain size of the alloy is coarse because of the high solution temperature, and it has good high temperature endurance and creep properties. Lower solution treatment temperature results in smaller grain size and higher tensile strength, fatigue strength and impact toughness. For example, when the solution temperature of GH4169 alloy varies from 940℃ to 1040℃, the tensile strength at room temperature decreases with the increase of the solution temperature, and the plasticity is very high. When the solution temperature ≥980℃, all the δ phase is dissolved, and the durable strength increases, but the durable plasticity decreases sharply.


The ni-base superalloy with low alloying degree generally needs only one aging treatment, while with high alloying degree, it often needs four stages of heat treatment, including two aging, three aging, and even two solid solution and two aging, to adjust the type, size and distribution of grain boundary precipitates once, and make the γ phase distribution more reasonable. Usually after a solution treatment, and then in the treatment of γ´ solution temperature below a time of aging. The second solution or first aging is also called intermediate treatment. The intermediate treatment can significantly increase the durable life and plasticity of superalloy and improve the microstructure stability of the alloy.



A few cast superalloys have high thermal strength and can be put into use after aging treatment. However, the coarse (γ+ γ´) eutectic exists in the as-cast microstructure of most of the high alloying cast superalloys. The γ´ phase has large particles, serious segregation and unstable microstructure. Therefore, high temperature solution treatment is necessary to improve the inhomogeneity of composition and microstructure of the alloy, and obtain a more reasonable distribution of the second phase, so as to improve the durable strength and creep strength of the alloy.


The disqualification of the permanent creep strength of superalloy is usually caused by the low solution treatment temperature and improper aging process, while the high solution treatment temperature will cause the decrease of the strength at room temperature and the decrease of the permanent plasticity. The properties of superalloys can be controlled in a wide range by adjusting the heat treatment process. It is particularly important to optimize the heat treatment process according to the service conditions of the workpiece.