Quenching treatment is carried out for medium and high carbon steel pipe (steel pipe mainly with low alloy steel or medium alloy steel) or for the emergency cooling method (water quenching) of Cr stainless steel tube.

As a result, high-strength steel tubes with high martensite ratios (specifically, martensite ratios of more than 80%) can be steadily manufactured.

The steel pipes containing high carbon alloy steels and Cr stainless steel are heated to A phase change point temperature, and water cooling is carried out from the outer surface of the steel pipe.

You can get the following (a) ~ (f) Insights.

(A) If the steel pipe is cooled by strong water quenching to the following martensite phase change stop temperature (Mf point), a high probability of quenching cracks is generated.

(B) Since the cracking of the quenching crack is roughly stretched in the shaft direction of the steel pipe, it can be considered that the main force for expanding the crack is the tensile stress in the circumference direction.

(C) With regard to the source of tensile stress in the preceding circumference, it can be considered that the temperature difference (uneven temperature) in the direction of the wall thickness generated during the cooling process leads to a deviation in the timing of martensite phase transition between the outer surface side of the steel pipe and the inner surface side.

(D) In particular, near the cooling surface with a large temperature unevenness (that is, a large temperature difference with the inner surface side), it is easy to produce microcracks based on brittle failure, which is easy to become the starting point of cracking and stretching.

(E) Cracking is, in most cases, stretched at the end of the steel pipe.

The reason can be considered to be that the stress increase coefficient at the end of the free surface is greater than that of the lower part of the end.

(F) In the case of water-cooled suppression of cooling speed, no quenching cracks are produced in the high carbon-containing low alloy steels and Cr stainless steel.
It should be explained that no quenching cracks are produced in the case of low alloy steels containing high carbon, inhibiting martensite and making the tissue of bainite body. In short, it can be considered that the quenching crack is based on the cracking of the end of the steel pipe with free surface as the starting point, the cracking is produced as a result of the development through Microcracks, the micro-crack is produced in the cooling process due to the temperature of the wall thickness of uneven thermal stress,

The tensile stress in the circumferential direction caused by the phase change stress (hereinafter referred to as "tensile stress" as "stress") also occurs near the cooling surface.

 

Methods For Preventing Quenching Cracks In Medium And High Carbon Low Alloy Steel Tubes