alloy steel

SA335 P91 Alloy Steel Pipe Welding Process Requirements

  • Tuesday, 24 December 2024
  • 0
  • 644
  • 0


The SA335 P91 alloy steel is a new steel type that adds an improved elements of v, Nb, N, Ti and Al  to the 9Cr-1Mo steel. The  alloy steel pipe has good anti-high temperature oxidation and creep resistance, and at the same time has good thermal strength, which can effectively reduce structural weight, so it is mainly used in power station equipment.
However, because P91 steel has a certain tendency of cold cracking and joint brittleness, so the welding process and heat treatment process have strict requirements.

P91 alloy steel except TIG welding, regardless of the thickness of the steel pipe, the preheating temperature needs at least 200 degrees C, and TIG welding, because of its very low diffusion hydrogen content, the preheating temperature can be relaxed to about 100-150 degrees C, the maximum temperature is generally limited to about 300 degrees C,
This ensures that each weld is converted into a margot tissue, resulting in partial tempering under the thermal cycle of the next weld. There are also some limitations to the choice of post-weld heat treatment temperature: this temperature must be higher than the minimum temperature specified by the various standards, i.e. above 730 degrees C, in practice, in order to obtain sufficient tempering of the weld metal, the actual treatment temperature is obviously required to be higher than this level (but not more than 780-790 degrees C).
In the actual welding practice, after 755 degrees C insulation 2-3h heat treatment, can obtain satisfactory impact toughness, but also to ensure that the hardness of the entire welding seam area is less than 300HV, weld metal hardness is generally 2402-280HV. Preheating is an effective way to prevent hot and cold cracks. German standards stipulate that the preheating and interlayer temperature should be 180-250 degrees C, not more than 350 degrees C, before heat treatment, the material must be cooled to 150 degrees C below, the stress is greater, the cold-de-cooling temperature should not be lower than 100 degrees C. If cooled at room temperature, moisture should be strictly prohibited. The preheating temperature of 150-350 degrees C is beneficial to the operation of the welder. At the same time, the welding current should be reduced appropriately to avoid arc pit cracks.

 

 