Effect of vanadium on microstructure and heat treatment of steel


(1)Vanadium and iron can form a continuous solid solution, strongly reduce the austenite phase area.

(2)Vanadium and carbon, nitrogen, oxygen have a strong affinity, mainly in steel carbide or nitride, oxide form.

(3) by controlling the austenitizing temperature to change the content of vanadium in austenite and the number of undissolved carbide and the actual grain size of steel, steel hardenability can be adjusted.

(4) because vanadium and carbon can form a stable refractory carbide, so that steel at a higher temperature still maintain fine crystal structure, greatly reduce the sensitivity of steel overheating.


The influence of vanadium on the mechanical properties of steel

(1) a small amount of vanadium can make the grain refinement, toughness increase.

(2) high content of vanadium leads to the appearance of concentrated carbide, so that the strength is reduced, carbide precipitation in the crystal will reduce the room temperature toughness, so in most steel content is not high.

When the carbide is dispersed and precipitated by proper heat treatment, vanadium can improve the high-temperature endurance strength and creep resistance of steel.

(4) vanadium carbide metal carbide is the hardest and most wear-resistant, dispersed carbide can improve the hardness and wear resistance of tool steel.


The influence of vanadium on the physical, chemical and technological properties of steel

(1) vanadium is added into fe-ni alloy, and the permeability can be improved after proper heat treatment. When vanadium is added to permanent magnetic steel, magnetic coercivity can be improved.

(2) add enough vanadium, carbon fixed in vanadium carbon compounds, can greatly increase the stability of steel under high temperature and high pressure to hydrogen, suitable for manufacturing reactors. Vanadium can improve the resistance to intercrystalline corrosion in stainless steel.

(3) vanadium oxide, the high temperature of steel oxidation resistance.

(4) vanadium steel in the lower processing temperature can significantly increase the deformation ability.

(5)Vanadium can improve the welding performance of steel