The Hazards Of Sulfur In Steel Pipe
Sulfur comes from the ore and fuel coke of steelmaking, which is a harmful element in steel. Sulfur is found in steel in the form of ferrous sulfide (FeS), FeS and Fe form a low melting point (985 degrees C) compounds, and steel heat processing temperature is generally at 1150-1200 degrees C, so when the steel is hot processed, FeS compounds will melt prematurely leading to the cracking of the steel tube, this phenomenon is called "thermal brittle."
The higher the sulfur content, the more serious the thermal brittle phenomenon, so the sulfur content in steel must be controlled. Advanced high-quality steel S 0.02-0.03%, high-quality steel S 0.03-0.045%, ordinary steel S 0.055%-0.07%.
In individual cases there may also be cases where sulfur is required, such as adding 0.08-0.20% sulfur to the steel, which can improve machinability, commonly referred to as easy-to-cut steel. Sulfur is also detrimental to welding performance and reduces corrosion resistance.