 The main reason of steel heat treatment deformation is the presence of internal stress or external stress in steel. The internal stress is caused by the uneven temperature distribution or phase change, and the residual stress is also one of the reasons. The deformation caused by external stress is mainly due to the "collapse" caused by the self-weight of the workpiece, and in special cases the workpiece heated by the collision should also be considered, or the SAG caused by clamping tool clamping, etc.

The change of workpiece size is mainly based on tissue transformation, so it shows the same expansion and shrinkage, but when there is holes or complex shape workpiece on the workpiece, it will lead to additional deformation.

2) Heating and deformation

During heating, the steel is converted from elastomer to plastic body around 450 ℃. The residual stress will also disappear due to recrystallization at about higher than this temperature. Therefore, when heating quickly, due to the temperature difference inside and outside the workpiece, the external reach of 450 ℃ into a plastic zone, and the internal temperature at the lower part of the residual stress is still deformed.

After cooling, the area is where the deformation occurs. When heating large workpieces, there is residual stress or uneven heating, can produce deformation. Residual stress mainly comes from the processing process.

When these stresses exist, due to the increase in temperature, the yield strength of the steel gradually decreases, even if the heating is very uniform, very slight stress will lead to deformation. Generally, the residual stress at the outer edge of the workpiece is higher, when the temperature rise from the outside, the outer edge of the deformation is larger, the faster the heating speed, the larger the size of the workpiece, the greater the change in the section, the greater the heating deformation.

Thermal stress depends on the uneven distribution of temperature and temperature gradient, which are the causes of the difference in thermal expansion. The phase change stress mainly originates from the unequal time of the phase change, that is, the phase change occurs in the part of the material, and the other parts are not produced when the phase change has occurred. When heated, the tissue transformation of the material austenite the volume shrinkage of the body can appear plastic deformation. If the same tissue changes occur in each part of the material at the same time, no stress is generated.

For this reason, slow heating can appropriately reduce the heating deformation, preferably using preheating.

3)Cooling and deformation

Thermal stress will occur when the cooling is uneven, resulting in deformation. Because of the difference of cooling speed between the outer edge and the interior of the workpiece, the thermal stress is inevitable, and the thermal stress is superimposed with the tissue stress under the quenching condition, and the deformation is more complicated.

In addition, the uneven organization, decarbonization, etc., will also lead to differences in phase change points, the expansion of phase change is also different.