Introduction To Steel Segregation
Severe inhomogeneity of steel composition is called segregation. This phenomenon includes not only the uneven distribution of common elements such as carbon, manganese, silicon, sulfur and phosphorus, but also the uneven distribution of gaseous and nonmetallic inclusions.
Segregation is caused by separation crystallization of molten steel during solidification. The purity of crystallized nucleus is high, and the impurity is left in the crystallized molten steel. Therefore, the crystal front of molten steel for carbon, sulfur, phosphorus and other impurities enrichment. With the decrease of temperature, impurity solidifies in dendrite or forms segregation zone. In addition, with the decrease of temperature, the solubility of gas in the molten steel decreases, and the gas is precipitated out at the crystal front and forms bubbles floating up. The molten steel enriched with impurities forms a strip segregation belt along the uphill track. Because the segregation appears in different parts on the ingot and in different forms on the low-power test plate, it can be divided into square segregation, "V", "^" shape segregation, point segregation, center segregation and intercrystalline segregation.
In addition, deoxidation alloying process improper operation, can cause serious uneven composition. The protective slag is involved in the molten steel, causing local carbonization. These factors often lead to a degree of segregation of steel more than that caused by separation crystallization.
Segregation affects the mechanical properties and corrosion resistance of steel. Severe segregation may cause brittle fracture of steel and damage of machinery during cold working, so segregation above the permitted level is not allowed.
The degree of segregation is often related to ingot type, steel type, smelting operation and casting conditions. The segregation of alloy elements, impurities and gases is more serious with the increase of casting temperature and casting speed. The segregation of continuous cast steel can be reduced by electromagnetic stirring. In addition, increasing the purity of molten steel is an important measure to reduce segregation.