Silicon element is added as reducing agents and deoxidizers in the steelmaking process, so killed steel will contain 0.15-0.30% of silicon, when the amount of silicon in steel exceeds 0.50-0.60%, then silicon is an alloy element. Silicon elements can significantly improve the elastic limit of steel, yield point and tensile strength, so it is widely used in spring steel, such as 65Mn and 82B spring steel contains 0.15-0.37% silicon.
Adding 1.0-1.2% silicon to the temperate structure steel can increase the strength of steel by 15-20%, silicon and tantalum, tungsten, chromium and other joints, which have the effect of improving corrosion resistance and antioxidant resistance, can manufacture heat-resistant steel, and low-carbon steel containing 1.0-4.0% of silicon, with very high magnetic conductivity, for the electrical industry to make tantalum steel sheet. Of course, silicon is not a profit-free, it will reduce the welding performance of steel pipe.