news
China's high temperature alloy rapid development
Superalloys, also known as heat-resistant alloys and superalloys, refer to metal materials with comprehensive properties such as creep resistance, high high temperature strength, good fracture toughness and corrosion resistance that work for a long time above 600 degrees Celsius and under a certain stress. Superalloy according to the matrix is divided into iron base, nickel base, cobalt base superalloy, iron base superalloy temperature is generally about 700 degrees Celsius, mostly used in transportation, petrochemical, mining metallurgy and other fields; Cobalt based superalloy is limited by the mining and use of cobalt, and has not been widely applied. Nickel-based superalloys can maintain good mechanical properties in harsh environments above 1000 degrees Celsius and are widely used in the manufacture of high-performance aerospace engines and the hottest end of industrial gas turbines. In addition, superalloys are divided into deformation, casting and powder superalloys according to the material forming method, and are divided into solid solution strengthened type, precipitation strengthened type, oxide dispersion strengthened type and fiber reinforced type superalloys according to the alloy strengthening method.
Since the development and production of superalloys began in 1956, more than 150 kinds of superalloys have been researched, trial-produced and produced. The domestic industrial layout has been basically formed, and the research and development and production system is relatively perfect, including scientific research units such as steel Research Institute Gaonar, Institute of Metals of the Chinese Academy of Sciences and 8 special steel plants such as Fushun Special Steel, Baowu Special Steel, Panchang Special Steel and Daye Special Steel; Related research and development technologies continue to make new breakthroughs, such as low segregation control technology, magnesium microalloying technology and other new technologies; The application field has been continuously expanded, in addition to the traditional aerospace and other sophisticated fields, the application range of superalloys in civilian fields such as smoke turbines and ground gas turbines has also gradually expanded.
With the rapid development of China's aerospace, nuclear power and other cutting-edge science and technology fields in recent years, coupled with the strong support of national policies, China's superalloy market is currently in strong demand, which not only promotes the steady growth of China's superalloy production, but also brings unprecedented development opportunities for the superalloy industry. According to published statistics, the demand for superalloy in China has increased rapidly from 30,000 tons in 2017 to 70,000 tons in 2022, with an average annual compound growth rate of 18.47%, while the production of superalloy in China has increased from 18,800 tons in 2017 to 42,000 tons in 2022, with an average annual compound growth rate of 17.44%; In 2023, the global superalloy market production and sales of 350,000 tons, China accounted for less than 1/10; In 2024, the demand for superalloy in China is 62,000 tons, an increase of 17%.


My company hot sale alloy seamless tubes
Boiler tubes,( 20G. 12Cr1MoVG, ASTM A335 P5, P9, P11),
ASTM A333 GR.6 seamless pipes, ( 1” to 24” sch40, sch80, sch160),
0users like this.