stainless steel
Classification Of Surface Corrosion Of Stainless Steel
Stainless steel due to its special metallographic structure and surface passivation film, it is more difficult to react with the media and corroded, but not under any conditions can not be corroded.
The following is a classification of two types of corrosion.
First, chemical corrosion
1, Surface pollution: attached to the surface of the workpiece oil, dust and acid, alkali, salt and so on in a certain condition into a corrosive medium, and stainless steel parts of some components of chemical reaction, resulting in chemical corrosion and rust.
2, Surface scratches: a variety of scratches on the passivation film damage, so that stainless steel protection capacity is reduced, easy to react with the chemical medium, resulting in chemical corrosion and rust.
3, Cleaning: Pickling passivation after cleaning caused by residual fluid retention, direct corrosion of stainless steel parts (chemical corrosion).
II. Electrical and chemical corrosion
1, Carbon steel pollution: in contact with carbon steel parts caused by scratches and corrosive media to form the original battery resulting in electrochemical corrosion.
2, Cutting: slag, splash and other easy to rust substances adhesion and corrosive media to form the original battery and produce electrochemical rot.
3, Roasting School: Flame heating area of the composition and metallographic structure changes and uneven, and corrosive media to form the original battery and produce electrochemical corrosion.
4, Welding: The welding area of physical defects (bite edge, stomata, cracks, non-fusion, not welded through, etc.) and chemical defects (grain size, grain boundary of poor chromium, segregation, etc.) and corrosive media to form the original battery and produce electrochemical corrosion.
5, Material: Stainless steel material chemical defects (uneven composition, S, P impurities, etc.) and surface physical defects (loose, sand eyes, cracks, etc.) are conducive to the formation of the original battery with corrosive media and the production of electrochemical corrosion.
6, Passivation: Pickling passivation effect is not good caused by uneven or thin stainless steel surface passivation film, easy to form electrochemical corrosion. 7, Cleaning: The retention of pickling passivation residue and stainless steel chemical corrosion of the production and stainless steel parts to form electrochemical corrosion.
0users like this.