stainless steel

Corrosion Analysis Of Stainless Steel Pipeline In Offshore Environment

  • Monday, 23 December 2024
  • 0
  • 561
  • 0


There are many differences between the Marine atmospheric environment and the inland atmospheric environment. When analyzing the corrosion of the stainless steel pipeline, it is necessary to consider the factors such as high temperature, high humidity, high salinity, sea breeze, salt spray and seawater splash.


1 High salt sea breeze, salt spray, sea splash

In the Marine environment of sea wind, waves are frequent, sea wind waves makes a lot of salt in the sea water caused by fluid mixed with air, make the atmosphere and a large amount of salt, and these lots of chloride ion in salt, the chloride ions in the salt has high conductivity, easy to form the electrolyte solution, formed in the metal surface micro batteries, enhanced the activity of the corrosion, damage the metal surface passivation membrane.

In the Marine environment, under the condition of high temperature, a large amount of seawater will produce atomization, forming a large amount of salt fog, and the main components of salt fog and sea water are very similar, on the surface of stainless steel pipe will also produce corrosion. The main cause of corrosion is the large number of chloride ions in the salt spray. The main form of corrosion of stainless steel pipe surface by salt spray is electrochemical corrosion. The electrochemical corrosion process of the salt spray on the stainless steel pipe is as follows: the salt spray contains a large number of sodium ions and chloride ions, and the corrosion of the salt spray on the surface of the stainless steel pipe is caused by a large number of chloride ions. Chloride ion has a strong penetration ability, which can easily penetrate the oxide layer and protective layer on the metal surface, and form electrochemical corrosion by electrochemical reaction with the metal interior. When the salt fog deposition to the surface of the stainless steel pipe, due to the salt fog there is a large amount of water vapor, first formed a brine membrane to cover the surface of the stainless steel pipe, then the surface of the stainless steel pipe is equivalent to immersed in sodium chloride solution containing oxygen, the surface of the stainless steel pipe will constitute the two poles of the galvanic cell, resulting in corrosion. Therefore, salt spray corrosion is different from saltwater corrosion in mechanism, and salt spray corrosion is higher.


2. High temperature and humidity environment

The temperature and humidity in the Marine environment are much higher than those in the inland environment. High temperature, high humidity environment makes sea water evaporation speed up, the evaporation of a large number of water vapor on the corrosion of stainless steel pipes. As a good medium, water vapor intensifies the transport speed of various ions and ACTS as a good corrosion medium. As the water carrying a large number of chloride ions penetrates into the pipeline, electrochemical corrosion or chemical corrosion occurs


3 Other factors

The impact of the waves played a role in stirring and renewing the electrolyte solution on the surface of the stainless steel pipe. Meanwhile, the erosion of the waves made the corroded rust layer fall off and accelerated the progress of corrosion. The growth of Marine organisms on the surface of the stainless steel pipeline can seriously damage the protective layer of the original object (such as the passivation film on the surface of the polished pipeline), so that the pipeline is damaged by corrosion. Meanwhile, the metabolites of Marine organisms (containing sulfide) further deteriorate the corrosive environment of the stainless steel pipeline, resulting in the aggravation of the corrosion effect. If the pipe is located in an acid rain area, the corrosion rate of the pipe is proportional to the PH value of acid rain.


Conclusion

On the premise that the material meets the requirements, the corrosion causes of stainless steel pipes in the complex Marine environment such as high temperature, high humidity, high salinity, sea breeze, salt spray and seawater splash are mainly chemical corrosion and electrochemical corrosion caused by chloride ions. The corrosion of stainless steel pipe can be inhibited or eliminated by changing the way of surface treatment, selecting materials with stronger corrosion resistance, surface coating of stainless steel pipe or electrochemical protection, etc.

Corrosion Analysis Of Stainless Steel Pipeline In Offshore Environment

0users like this.

Leave a Reply