1.Definition of solid-soluble reinforcement

The alloy element is dissolved in the substrate metal to cause a certain degree of lattice distortion, thus increasing the alloy strength.
2. Principles

The solute atoms dissolved into the solid solution cause the lattice distortion, the lattice distortion increases the resistance of the misalignment motion, making the slip-up difficult to carry out, thus increasing the strength and hardness of the alloy solid-soluble. This phenomenon of solid-soluble body by dissolving into a certain solute element is called solid-soluble reinforcement.
When the concentration of solute atoms is appropriate, the strength and hardness of the material can be improved, while its toughness and plasticity are reduced.

3. Major factors in the degree of solid-dissolving reinforcement

The difference in size between the base and the solute atom.
The greater the size difference, the greater the interference to the original crystal structure and the more difficult it is to slip.

The amount of alloying elements. The more alloying elements are added, the greater the reinforcement effect. If too many atoms are added, it will exceed the solubility.
This involves another strengthening mechanism, decentralized phase strengthening.
The interstitial solute atom has a greater solid-soluble reinforcement effect than the displaced atom.
The greater the difference between the valence of solute atoms and the number of valuing metals, the more significant the solid-soluble reinforcement.

 

 