steel pipe
Application Range Of Centrifugal Casting Bimetallic Composite Pipe
Centrifugal Casting bimetallic Composite pipe is the centrifugal variable speed casting, internal and external layers of low melting point adiabatic flux washing slag, inert gas protection and other processes to achieve two kinds of metal composite, the formation of finished sets, rollers or composite tube billet, less defects, high bonding strength, easy to connect and repair, high quality, at the same time low cost. The main application range is:
1, corrosion-resistant pipeline tube high H2S/CO2 oil and gas field corrosion environment is bad, the ground pipeline corrosion is serious, x52ns/2205 or x60/825 bimetallic Composite pipe use, provides a solution to the surface pipeline corrosion problem effective way,
Both technically and economically, the advantages are obvious.
2, wear-resistant conveyor pipe cement conveyor and drilling pump cylinder liner in the requirements of high wear resistance at the same time, must have a good strong toughness, but also can meditate between the pipe segment of the group welding, the whole pipeline to play a supporting role.
It can not only realize the performance potential of the two materials, improve the comprehensive performance, but also reduce the production cost and improve the economic benefit by using the double metal metallurgical composite pipe with external pressure.
3, Boiler tube metallurgy fusion centrifugal billet extrusion cold rolling 304l/cr.a-1 composite pipe was successfully used in the boiler manufactured by Dongfang Boiler Co., Ltd., replacing the external corrosion resistance of the thermal expansion of the heat amplification with the mechanical composite pipe, and for the metallurgical bimetallic Composite steel pipe double-layer interface flaw detection developed the corresponding ultrasonic testing operating procedures.
4, composite roll using centrifugal composite casting method to produce bimetallic composite roll, with external working layer density, less casting defects, good mechanical properties and high hardness of the surface wear-resistant layer, long service life, high production efficiency characteristics.
BEIJING China Metallurgical Equipment Research Institute design General Hospital using centrifugal composite method in φ900mmx1800mm vertical centrifuge prepared φ275mmx400mm high chromium cast iron/gray iron composite roll.
5, other through centrifugal casting, extrusion production with metallurgical fusion layer of bimetallic composite pipe, in the requirements of pipeline corrosion resistance, wear-resistant, pressure-resistant petroleum, chemical, boiler industry has been the application space.

0users like this.