Automatic rolling process is one of the production methods of seamless steel pipe.

Production equipments include piercing mill, automatic pipe rolling mill, fixed diameter machine and slight reduction mill and so on. 

The circular tube billet is rolled into a hollow thick wall tube (application), and the axis of two rolls and the rolling line form a tilt angle. In recent years, the tilt angle has been increased from 6°~12° to 13°~17°, which accelerates the perforation speed. Production of more than 250mm diameter steel pipe, the use of two perforation, in order to reduce the wall thickness of the tube. 

 New processes such as perforation of active rotating guide plate, thrust perforation after band, axial discharge and cyclic top welding have also achieved some development, thus strengthening the perforation process and improving the quality of capillary tube. Generally through the 2~3 road, rolling to the finished wall thickness, the total elongation is about 1.8~2.2. 

Since the 70 's, the production efficiency has been improved and the mechanization of rolling pipe has been realized by using the techniques of single hole groove roll, double rack serial rolling mill, double groove tracking rolling and spherical head. The purpose of homogenization is to eliminate the defects of internal and external surfaces and the ellipticity of waste tubes, and to reduce the uneven thickness of transverse walls. 

 In recent years, three rollers are used to improve the deformation and homogenization efficiency of the whole machine.

The diameter reducer is composed of 3~12 frame, and the diameter reduction machine is composed of 12~24 frame, and the reduction rate is about 3~28%. The tension reducer, which appeared in the 50 's, controls the wall thickness with appropriate tension while adjusting the roll speed and reducing the diameter. The new tension reducer generally uses three-roll type, has the 18~28 frame, the maximum reduction rate is 80%, the wall reduction rate is 44%, the outlet speed is 18mm per second. 

Tension reduction machine has the disadvantage of thickening at both ends, can be used "head and tail end of the sudden plus electrical control" or micro-tension reduction path elimination. Automatic pipe rolling mill commonly used series have outer diameter of 100mm, 140mm, 250mm and 400mm four kinds, the production of outer diameter 17~426mm steel pipe. The characteristic of the unit is to realize the main deformation on the piercing machine, the specification change is more flexible, the production variety is wide range. 

   Due to the development of continuous rolling pipe technology, the construction of units below 140mm is no longer built.