According to the analysis of the production process, the factors that affect the friction between the inner wall of the steel tube and the inner mould are mainly the lubrication, and also the plasticity of the steel tube. If the steel tube has poor plasticity, the possibility of drawing cracking will be greatly increased, and the poor plasticity is obviously related to the intermediate stress removal annealing. In addition, due to the small opening degree of the crack and no obvious signs of expansion, it is indicated that the crack has not experienced the influence of secondary drawing deformation after its formation. Therefore, it is further inferred that the most likely time for the formation of the crack should be the second cold drawing process. The most likely influencing factors are poor lubrication and poor desorption annealing.

Through a series of tests, it is fully verified that lubrication and intermediate stress relief annealing in the process of cold drawing of steel tube have a crucial effect on the quality of finished steel tube.

Through comparative analysis, it shows that the poor lubrication + no intermediate annealing treatment and poor lubrication, intermediate annealing temperature is low in both cases, all can produce transverse crack, and poor lubrication in + intermediate annealing is good, good lubrication, no intermediate annealing treatment and good lubrication + intermediate annealing temperature on the low side, although can produce jutter defects, but does not cause steel tube wall transverse cracks. Obviously, poor lubrication is the main cause of transverse crack, and poor intermediate stress removal annealing is the secondary cause.

 

Causes Of Transverse Cracks In The Inner Wall Of Cold-Drawn Seamless Steel Tube

Causes Of Transverse Cracks In The Inner Wall Of Cold-Drawn Seamless Steel Tube

0users like this.

Leave a Reply

RSS

Get in touch

Refresh Code