Steel pipe varieties are numerous, the steel grade (species) is also different, the same variety of steel pipe may also have some differences in its chemical composition, but after heat treatment steel pipe can meet the relevant technical standards or the procurement side of the technical conditions.
According to product standards, steel pipe heat treatment process mainly has the following 5 categories.

(1) Quenching + high-temperature tempering (Q+T, also known as tempering treatment): Heating the steel pipe to the quenching temperature, so that the internal tissue of the steel pipe into austenite, and then with a rapid cooling at greater than the critical quenching speed, so that the internal tissue of the steel pipe into martensite, and then with high temperature tempering, and finally make the steel pipe tissue

Quenching + tempering can not only improve the strength and hardness of steel pipe, but also combine the strength, plasticity and toughness of steel pipe organically to meet the requirements of the purchaser for steel pipe performance.

(2) Normalization (N): Heat the steel pipe to the positive fire temperature, so that the internal tissue of the steel pipe is completely transformed into austenitic tissue, the air as the medium for cooling heat treatment process. Different metal tissues, such as pearlite, Bainite, Martensite, or their mixed tissues, can be obtained after the fire.

The positive fire can not only refine grain, uniform composition and eliminate stress, but also improve the hardness of steel pipe and improve its cutting performance.

(3) Normalization + tempering (N+T): Heat the steel pipe to the positive fire temperature, so that the internal tissue of the steel pipe is completely transformed into austenitic tissue, cooling in the air, and then with the tempering process. Steel pipe tissue is tempering ferrite + pearlite, or ferrite + bainite, or tempering bainite, or tempering martensite, or tempering solitic.

The hot treatment process system can stabilize the internal microstructure of steel pipe and improve the plasticity and toughness of steel pipe.

(4) Annealing: Heating the steel pipe to the annealing temperature and insulation for a certain period of time, with the furnace slowly cooled to a certain temperature after the cooling of a heat treatment process. The annealing process of steel pipe can be divided into: spheroidization annealing, Complete annealing, de-stress annealing and so on.

The main role of Steel pipe annealing: ① Reduce the hardness of steel pipe, improve its plasticity, in order to facilitate subsequent cutting or cold deformation processing; ② refine grains, eliminate tissue defects, uniform internal tissues and components, improve the performance of steel tubes or prepare for subsequent processes; ③ eliminate internal stresses of steel tubes to prevent deformation or cracking.

(5) Solid solution treatment (mainly used in the production of type 18-8 austenitic stainless steel): Heat the steel pipe to the solid solubility temperature, so that carbide and various alloy elements fully evenly dissolve in the Huo body, and then quickly cool, so that carbon and alloy elements too late to precipitate, access to a single austenitic tissue heat treatment process. The main functions of solidification treatment: The internal organization of ① uniform steel pipe, the composition of uniform steel pipe; ② eliminates hardening during processing to facilitate subsequent cold deformation processing; ③ restores the corrosion resistance of stainless steel.

 