During the smelting process of steel, the deoxidization reaction will produce oxides and other products. If these products do not emerge before the solidification of the molten steel, they will remain in the steel. When the oxygen, sulfur, nitrogen and other impurities dissolved in the molten steel are cooled and solidified, or the solid solution is precipitated, and finally remain in the ingot.

The distribution of endogenous inclusions is relatively uniform and the particles are small. Correct operation and reasonable technological measures can reduce the number and change the composition, size and distribution, but it is generally inevitable.


2. Foreign inclusions

Slag suspended on the surface of molten steel during the smelting and pouring process, or refractory materials or other inclusions spalling from the inner wall of the furnace, steel tank and ladle, etc. are not removed in time before the solidification of molten steel and remain in the steel. It is the inclusion of metal in the melting process with the external material interaction.

The general characteristics of such inclusions are irregular shape, large size, and irregular, also known as coarse inclusions. Such inclusions can be avoided by proper handling.


Classification by chemical composition:


Class A (sulfide) : A single gray inclusion with A high ductility and A wide range of morphology, generally with rounded ends.

Class B (alumina) : mostly undeformed, angular, shape smaller than (generally < 3), black or bluish particles, arranged in a row along the rolling direction, with at least 3 particles.

Class C (silicates) : single black or dark gray inclusions with high ductility, having a wide range of morphologies (generally ≥3), generally with sharp ends.

Class D (globular oxides) : nondeformable, angular or rounded, smaller than (generally < 3), black or bluish, irregularly distributed particles.

Ds class (single particle globular class) : round or nearly round gallbladder particle inclusions with diameter ≥13 x m


Concept And Classification Of Nonmetallic Inclusions In Steel