Factors Affecting Yield Strength Of Steel
The internal factors that affect the yield strength of steel are: binding bond, organization, structure, atomic nature.
If the yield strength of metal is compared with ceramics and polymer materials, it can be seen that the influence of bonding bond is fundamental.
In terms of the impact of the organizational structure, there can be four reinforcement mechanisms that affect the yield strength of metallic materials, which is:
(1) Solid solubility enhancement;
(2) deformation enhancement;
(3) Precipitation enhancement and dispersion enhancement;
(4) Grain boundary and microcrystalline reinforcement. Precipitation strengthening and fine crystal reinforcement are the most commonly used methods to improve the yield strength of materials in industrial alloys.
Among these reinforcement mechanisms, the first three mechanisms, while improving the strength of the material, also reduce the plasticity, only the refinement of grain and amorphous, can not only improve the strength but also increase the plasticity.
The external factors affecting yield strength are: temperature, strain rate and stress state.
With the decrease of temperature and the increase of strain rate, the yield strength of the material increases, especially the body heart cubic metal is particularly sensitive to temperature and strain rate, which leads to the low temperature brittleness of steel. The effect of stress state is also important. Although yield strength is an essential index to reflect the intrinsic properties of the material, the stress state is different and the yield strength value is different. The yield strength of the material we usually refer to is generally the yield strength when stretching in one direction.