steel pipe
Factors Leading To Deformation Of Steel By Heat Treatment
1. Carbon content and its influence on heat treatment variation
The deformation of high carbon steel is smaller than that of medium carbon steel when the yield strength is increased. For carbon steel, the deformation of T7A steel is minimal in most cases. When the mass fraction of carbon is greater than 0.7%, it tends to shrink. However, when the mass fraction of carbon is less than 0.7%, both inner and outer diameters tend to expand.
The yield strength of carbon steel itself is relatively low, so the carbon steel part with inner hole (or cavity) has larger deformation, and the inner hole (or cavity) tends to swell. Due to the high strength, low Ms point and large residual austenitic volume of alloy steel, the quenching deformation is small, which is mainly manifested as the thermal stress deformation, and the inner hole (or cavity) of the steel parts tends to shrink. Therefore, when quenched under the same condition as medium carbon steel, the workpiece of high carbon steel and high alloy steel is usually dominated by shrinkage of internal hole.
2. Influence of alloy elements on heat treatment deformation
The influence of alloying elements on the heat treatment deformation of workpiece is mainly reflected in the influence on the Ms point and hardenability of steel. Most alloying elements, such as manganese, chromium, silicon, nickel, molybdenum, boron, etc., reduce the Ms point of steel, increase the volume of residual austenitic, reduce the specific volume change and microstructure stress of steel during quenching, and therefore, reduce the quenching deformation of the workpiece. Alloying elements significantly increase the hardenability of steel, thereby increasing the volume deformation and microstructure stress of steel, resulting in the increase of the workpiece heat treatment deformation tendency. In addition, due to the alloy element to improve the hardenability of steel, so that the critical quenching cooling speed is reduced, the actual production, can be used to moderate the quenching medium quenching, so as to reduce the thermal stress, reduce the heat treatment deformation of the workpiece. The influence of silicon on the Ms point is not significant, and it only reduces the deformation of the sample. Tungsten and vanadium have little effect on hardenability and Ms point, and have little effect on heat treatment deformation of workpiece. Therefore, the so-called micro-deformed steel in industry contains a large amount of silicon, tungsten, vanadium and other alloying elements.
3. Influence of original structure and stress state on heat treatment deformation
The original structure of the workpiece before quenching, such as the shape, size, quantity and distribution of carbide, the segregation of alloying elements, and the direction of fiber formed by forging and rolling all have certain influence on the heat treatment deformation of the workpiece. The spherical pearlite is larger in size and stronger than the flake pearlite, so the quenching deformation of the workpiece which has been spheroidized in advance is relatively small. For some high carbon alloy tool steels, such as 9Mn2V, CrWMn and GCr15, the spheroidization grade has a great influence on the correction of heat treatment deformation cracking and post-quenching deformation. Generally, grade 2.5-5 spheroidization is preferred. Quenching and tempering not only reduces the absolute value of the workpiece deformation, but also makes the quenching and tempering of the workpiece more regular, which is conducive to the control of deformation.
The strip carbide distribution has a great influence on the heat treatment deformation of the workpiece. After quenching, the workpiece expands in the direction parallel to the carbide strip, and contracts in the direction perpendicular to the carbide strip. The morphology and distribution of carbides have a significant influence on quenching deformation of Cr12 steel and high speed steel.
In short, the more uniform the original structure of the workpiece, the smaller the heat treatment deformation, the more regular the deformation, the more easy to control.
4. The stress state of the workpiece itself has an important influence on the deformation before quenching. In particular, if the residual stress is not eliminated, it has a great influence on the quenching deformation of the workpiece with complicated shape and large feed.
5. Influence of workpiece geometry on heat treatment deformation
The workpiece with complex geometry and asymmetric cross-section shape, such as the shaft with keyway, keyway broach, tower workpiece, etc., dissipates heat quickly on one side and slowly on the other side during quenching and cooling, which is a kind of uneven cooling. If the above caused by uneven cooling in Ms deformation predominates, is cooled fast side concave, if under Ms of deformation caused by the uneven cooling box, is cooled fast one side convex, increase the isothermal time, growth amount of bainite transformation, the residual austenite is more stable, reduce the amount of martensitic transformation in the air cooling, can significantly reduce the workpiece deformation.
6. Influence of process parameters on heat treatment deformation
Both conventional heat treatment and special heat treatment may produce heat treatment deformation. When analyzing the influence of heat treatment process parameters on heat treatment deformation, the most important thing is to analyze the influence of heating process and cooling process. The main parameters of heating process are heating uniformity, heating temperature and heating speed. The main parameters of cooling process are cooling uniformity and cooling speed. The influence of non-uniform cooling on quenching deformation is the same as that of the non-uniform cooling caused by the shape asymmetry of the workpiece section. This section mainly discusses the influence of other process parameters.
0users like this.