Heat Treatment Defects Of Steel Tube And Its Prevention
Heat treatment of metal materials is divided into whole heat treatment, surface heat treatment and chemical heat treatment. Heat treatment of steel tube generally adopts whole heat treatment. Generally through the heating, insulation, cooling and other basic processes, these processes are likely to produce defects.
The heat treatment defects of steel tube mainly include the unqualified structure of steel tube, the size exceeding the standard and surface crack, abrasion, severe oxidation, decarbonization, overheating and over burning.
The microstructure and properties of steel tube are unqualified:
Pearlite, Bainite and martensite can be obtained after austenite of steel tube according to different carbon content and cooling rate. If the heat treatment process is not properly controlled, the organization may be produced. The organization of Wei is an overheated organization. It has a bad effect on the comprehensive performance of the steel pipe (the organization is superior to the high temperature durability), which can reduce the normal temperature strength and increase brittleness. The lighter bodies of the Organization can be eliminated by proper temperature, and the more severe of the organization can be eliminated by two times of positive fire. The first normalizing temperature is higher and the second normalizing temperature is lower. It also plays a role in grain refinement.
After heat treatment of steel tube, in some cases its size will change significantly, including the diameter of the steel tube, the degree of ellipse and the variation of the curvature. Generally occurs when the quenching process. The process of sizing is often added after tempering. The variation of the ellipse of the steel tube usually occurs at the end of the steel pipe, mainly because the tube end is "burnt down" due to the long time heating of the large diameter thin-walled tube.
Generally speaking, the bending of steel pipe can be corrected by straightening machine. When the bending degree is very big, can cause the steel pipe to transport the difficulty, in straightening the steel pipe will produce the very big straightening stress. Will seriously reduce
Anti-crush performance and corrosion resistance of low steel pipe. What's more, the steel pipe in the straightening process occurs in the straightening or straightening.
Surface crack of steel pipe
In the process of heat treatment of steel tube, excessive temperature stress will cause surface crack of steel pipe. The surface crack of steel tube is mainly caused by heating speed or too fast cooling rate. When the high alloy thick wall tube is heated, if the heating furnace temperature is too high, the steel pipe enters into the stove to encounter the quick heating, it is easy to produce the big temperature stress, tends to crack. In order to reduce the heat treatment crack of the steel pipe, we should make different heating system according to the steel grade and choose the appropriate quenching medium. On the other hand, the quenched steel tube should be tempered or annealed as soon as possible to eliminate residual stress.



Galaxy Company Hot Sale Steel Pipe Products:
OCTG, casing, tubing, seamless steel pipe, line pipe, boiler tube, ASTM A333 pipe, ASTM A335 alloy pipes, Mechanical pipe, API 5L pipe,, welded steel pipe,Galvanized pipe, SSAW pipes, LSAW pipes, steel pipe inventory, Chinese pipe factory, API 5L X52 pipe, pipe fittings, API 5CT pipe, Steel pipe, stainless steel pipes. ASTM A213 boiler tube