The Heat treatment of metal materials is divided into whole heat treatment, surface heat treatment and chemical heat treatment. Heat treatment of steel tube generally adopts whole heat treatment. 

Generally through the heating, insulation, cooling and other basic processes, these processes are likely to produce defects. 

The heat treatment defects of steel tube mainly include the unqualified structure of steel tube, the size exceeding the standard and surface crack, abrasion, severe oxidation, decarbonization, overheating and over burning. Heat treatment process characteristics of steel tube: The first process is heating: One is the critical point Ac1 or AC3 below the heating, the other is the critical point Ac1 or Ac3 above the heating. 

The first is to stabilize the structure of steel and eliminate residual stress of steel pipe, the second is mainly to steel austenite. 

The second procedure is heat preservation: the aim is to get the heating temperature of the uniform steel pipe to obtain a reasonable heating organization. The third process is cooling: cooling process is the key process of heat treatment of steel tube, he decided that the steel tube after cooling metallographic microstructure and mechanical properties. The cooling methods of steel tubes used in the actual production process are various. Often used cooling methods are furnace cooling, air cooling, oil cooling, polymer cold, water-cooled.

According to different heating temperature of steel tube, combined with different cooling rate of steel tube, it is divided into normalizing, annealing, tempering, quenching and other processes. Normalizing: Refinement of austenite grain, uniform internal structure and change of residual stress State, improve the comprehensive performance of steel pipe. To reduce the formation of steel tube in the deformation process of banded structure and mixed crystal (but not to eliminate the segregation in the steel and the inclusions caused by the banded tissue); To eliminate the reticular carbide in the hypoeutectoid, which is propitious to spheroidization annealing, is used as pretreatment before quenching of medium carbon steel and alloy structure, so as to refine the grains to make the microstructure homogeneous, 

Reduce the pipe defects produced by quenching process, for low carbon steel and low alloy steel pipe to replace annealing, improve the cutting performance of steel pipe, also can be used as the final heat treatment of ordinary steel pipe. Annealing: It is divided into recrystallization annealing, complete annealing, isothermal annealing, spherical annealing and elimination of residual stress annealing. 

General high carbon, low alloy and alloy steel pipe, the need to reduce its hardness and strength by annealing, improve plasticity, eliminate internal stress and uneven organization, refinement of crystalline microstructure, in favor of the machining of steel pipe and the final heat treatment for steel pipe laying the foundation. Tempering, generally divided into low-temperature tempering (150-250°c), medium temperature tempering (350-500°c), and High-temperature tempering (500-650°c). To improve the plasticity and toughness of the steel pipe, so that the steel pipe to obtain good comprehensive mechanical properties, reduce or eliminate the steel pipe in the quenching of residual stress and stabilize the steel pipe size, so that the steel pipe in the use of the process does not change. 

Tempering generally use air cooling, in order to prevent the steel pipe to produce internal stress, should be slow cooling; for high-temperature tempered brittle steel pipe, after tempering should be used for rapid cooling, such as oil cold. Quenching: The metal material heats up to the austenite Ac3 line above 30-50°c, after the heat preservation time causes the steel tube to cool quickly and obtains the martensite or the Bainite the craft process. Heat stress and tissue stress can be produced after quenching of steel tube, which is usually eliminated and improved by tempering. 

The combination of quenching and tempering (quenched and tempered) can make the comprehensive performance of steel greatly improved. Other processes, such as solid solution treatment and protection of gas heat treatment.