1. Overheating

We know that overheating in the heat treatment process is most likely to lead to the thickening of austenite grains, so that the mechanical properties of parts decline.

The heating temperature is too high or the holding time at high temperature is too long, resulting in austenite grain coarsening called overheating. The coarse austenite grain will reduce the strength and toughness of steel, increase the brittleness transition temperature and increase the deformation and cracking tendency during quenching. The cause of overheating is the loss of control of the furnace temperature meter or mixing (often do not understand the process). The superheated structure can be re-austenized to refine the grain under normal conditions after annealing, normalizing or multiple tempering at high temperature.

After re-heating and quenching, the superheated steel can refine the austenite grain, but sometimes there are still coarse granular fracture. It is generally believed that debris such as MnS was dissolved into austenite and enriched in grain interface due to high heating temperature. However, when cooled, these inclusions would be precipitated along grain interface, and it is easy to fracture along coarse austenite grain boundary under impact.

2. Over-burning phenomenon

Excessive heating temperature will not only lead to coarse austenite grains, but also lead to partial oxidation or melting of grain boundaries, leading to weakening of grain boundaries, known as overburning. The properties of steel deteriorate seriously after overfiring and crack is formed during quenching. Burned tissue cannot be recovered and can only be scrapped. Therefore in the work to avoid the occurrence of overheating.

3. Decarburization and oxidation

When steel is heated, carbon in the surface layer reacts with oxygen, hydrogen, carbon dioxide and water vapor in the medium (or atmosphere), reducing the carbon concentration in the surface layer, called decarburization.

Heating, steel surface of iron and alloy and elements and medium (or atmosphere) in oxygen, carbon dioxide, water vapor and other reactions to form oxide film called oxidation. High temperature (generally more than 570 degrees) after the oxidation of the workpiece dimensional accuracy and surface brightness deterioration, with poor hardenability of the oxidation film steel easy to appear quenching soft point.

In order to prevent oxidation and reduce decarburization measures include: workpiece surface coating, sealed heating with stainless steel foil package, heating with salt bath furnace, heating with protective atmosphere (such as purified inert gas, control of carbon potential in the furnace), flame combustion furnace (making furnace gas reductive)

4. Hydrogen embrittlement

Hydrogen embrittlement is the phenomenon that the plasticity and toughness of high strength steel are reduced when heated in hydrogen rich atmosphere. The workpiece with hydrogen embrittlement can also eliminate hydrogen embrittlement by removing hydrogen processing (such as tempering, aging, etc.), and hydrogen embrittlement can be avoided by heating with vacuum, low hydrogen atmosphere or inert atmosphere.

 

Heating Defects And Control In Heat Treatment Of Steel Pipes

0users like this.

Leave a Reply

RSS

Get in touch

Refresh Code