Steel forging crack generally formed in high temperature, forging deformation due to the crack expanding and exposure to air, when in 100 or 500 x x microscope, visible in the crack filling scale, and both sides is decarburization, organization for ferrite, its morphology is crack is thick and the commonly exists in the form of multiple, no detail tips, more pure, no detail orientation, divided by the number In addition to the typical shape, some forging cracks are sometimes finer. Instead of full decarbonization around the crack, it is semi-decarbonization.

The cracks produced during quenching heating are obviously different from those produced during forging heating in terms of properties and morphology. For structural steel, the heat treatment temperature is generally much lower than the forging temperature, even for high speed steel, high alloy steel, its heating and holding time is far less than the forging temperature. Due to the high heating temperature of heat treatment, too long holding time or rapid heating, early cracking will occur in the heating process. Cracks along coarse grain boundaries are produced. Both sides of the crack slightly decarbonized structure, parts heating speed is too fast, will also produce early cracking, this crack on both sides of no obvious decarbonization, but the crack and its tail filled with oxide skin. Sometimes because of high temperature instrument failure, the temperature is very high, resulting in the parts of the organization is very coarse, its cracks along the coarse grain boundary distribution.

Raw material cracks, for the same batch of the same type of workpiece, material cracks may not be repeated in the same location, the depth of the microscope is different. The material cracks are mostly consistent with the longitudinal direction of the material.


Identification Of Steel Forging Crack, Heat Treatment Crack And Raw Material Crack

0users like this.

Leave a Reply

RSS

Get in touch

Refresh Code