steel pipe

Inner Fold Of Seamless Steel Pipe

  • Tuesday, 24 December 2024
  • 0
  • 378
  • 0


The inner fold of steel seamless pipe is divided into two categories: steel inner fold and operation internal fold. 

1 The inner fold of the steel seamless pipe is irregularly distributed flake folding and helical folding, and the edge of the defect is mostly jagged. 

It is generally caused by the residual shrinkage and intermediate loosening of the billet. 

2 Operation Internal folding

Operation of the main form of mesh, dot shape, flake, spiral and so on. The regular spiral defect is usually caused by the serious head wear or the core rod defect, this kind of defect in addition to the regular distribution, the defect edge is neat than the steel defect. 

Irregular mesh, point shape, flake and other internal fold defects are generally caused by the following reasons. 

① The amount of pressure is too large, causing the Tube billet to form a orifice cavity prematurely during perforation, resulting in internal folds. 

② In the Tube billet, heating uneven and heating temperature is too high, easy to cause internal folding. 

③ The perforation after the appearance of the "Big ear" did not cut off, pre-wear the core rod will be "large ear" into the wool tube caused by the internal fold, this fold is flaky, generally appear in the tail section


0users like this.

Leave a Reply

RSS

Get in touch